1-20 of 431 Search Results for

bulk forming process

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400001
EISBN: 978-1-62708-316-4
...Abstract Abstract This chapter provides an introduction to metal forming processes and where they fit among the five general areas of manufacturing. It also discusses the basic differences between bulk deformation and sheet-metal forming processes and how they relate to hybrid forming processes...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730139
EISBN: 978-1-62708-283-9
...Abstract Abstract This chapter describes the processes, applications, and limitations of forming and shaping various materials. It discusses bulk forming, hot working, cold working, sheet forming, and polymer and powder processing. bulk forming cold working hot working polymer...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240279
EISBN: 978-1-62708-251-8
..., sheet metal forming processes, blanking and piercing, bending, stretch forming, drawing, rubber pad forming, and superplastic forming. hot working cold working bulk deformation rolling forging extrusion sheet metal forming blanking piercing bending stretch forming drawing rubber pad...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... Fig. 29 Oxide layer of 6 μm, indicative of Fe 3 O 4 obtained on reduction of the steam treatment temperature to 530 °C Abstract Abstract This chapter reviews failure aspects of structural ferrous powder metallurgy (PM) parts, which form the bulk of the PM industry. The focus...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040091
EISBN: 978-1-62708-300-3
... of Three-Dimensional Finite Element Modeling in Bulk Forming Processes, ” J. Mater. Process. Technol. , Vol 113 , 2001 , p 40 –45. 10.1016/S0924-0136(01)00590-8 [Thomsen et al., 1954] Thomsen E.G. , Yang C.T. , Bierbower J.B. , “ An Experimental Investigation of the Mechanics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.9781627082839
EISBN: 978-1-62708-283-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
.... , and Knight W. , Product Design for Manufacture and Assembly , Marcel Dekker, Inc. , 1994 6.2 Schey J.A. , Introduction to Manufacturing Processes , McGraw-Hill Book Co. , 1987 6.3 Kuhn H. , Design for Deformation Processing , Metalworking: Bulk Forming , Vol 14A , ASM...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040059
EISBN: 978-1-62708-300-3
... V. , Ed., Plenum Publishing , 1978 , p 113 – 120 . 10.1007/978-1-4613-4024-9_3 [Semiatin et al., 1987] Semiatin S.L. , Collings E.W. , Wood V.E. , Altan T. , “ Determination of the Interface Heat Transfer Coefficient for Non-Isothermal Bulk-Forming Processes, ” Trans...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040193
EISBN: 978-1-62708-300-3
... on Engineering Systems Design and Analysis , Montpellier, France , 1996 . [Wu et al., 2001] Wu W.T. , Oh S.I. , Arimoto K. , “ Recent Developments in Process Simulation for Bulk Forming Processes, ” Journal of Materials Processing Technology , Vol. 111 , 2001 , p 2 – 9 . 10.1016/S0924...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230145
EISBN: 978-1-62708-298-3
... Metall. , Vol 27 ( No. 11 ), p 1727 – 1747 10.1016/0001-6160(79)90087-7 Xiao X. , Fang S. , Wang G. , Hua Q. , and Dong Y. , 2004 . Influence of Beryllium on Thermal Stability and Glass-Forming Ability of Zr-Al-Ni-Cu Bulk Amorphous Alloys , J. Alloy. Compd. , Vol...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030126
EISBN: 978-1-62708-282-2
... and microstructure and SCC is equally as complex as the relationship between the environment and SCC. Bulk alloy composition can affect passive film stability and phase distribution (for example, chromium in stainless steel), minor alloying elements can cause local changes in passive film-forming elements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
... is the roughness of the counterface. For rough and hard counterfaces, the wear mode is generally that of bulk or cohesive wear. Interfacial wear is initiated only when the counterface is smooth enough to form interfacial junctions between the polymer and the counterface. An excellent example of interfacial wear...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... ). That is, the cold spray process can produce numerous forms of thick deposit up to almost bulk scale with good mechanical properties, and the manufacturing time can be much reduced by leaving out the unnecessary bonding process between the final product components. Cold spray thus has great potential...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090001
EISBN: 978-1-62708-266-2
... of the advancing crack Chemical reactions in the bulk The rate of interatomic bond rupture Fig. 1.5 Schematic of crack-tip processes that may be the rate-determining step in environmentally assisted crack propagation. For this illustration, an internal hydrogen embrittlement mechanism is assumed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460185
EISBN: 978-1-62708-285-3
... that was formed. The feedstock powder for LPPS and cold spray trials was in the size range of 5 to 37 μm. The smoother surface of the cold-sprayed coating is explained by the fact that the coarser fraction of the feedstock particles did not take part in the deposition process. The coarser particles do not exceed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
... molding compound consisting of chopped strands of glass fiber in combination with a resin, in either sheet form (sheet molding compound) or bulk form (bulk molding compound). A “charge” of these compounds is placed in a matched metal mold and cured under heat and pressure. During cure the material flows...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.9781627083553
EISBN: 978-1-62708-355-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
...Abstract Abstract This chapter discusses the properties and processing characteristics of glass, aramid, carbon, and ultra-high molecular weight polyethylene fibers and related product forms, including woven fabrics, prepreg, and reinforced mats. It also includes a review of fiber terminology...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420263
EISBN: 978-1-62708-310-2
... the experimentally observed bulk glass-forming range. Source: Ref 13.2 Fig. 13.5 Critical diameters of the cast glassy rods as a function of the titanium concentration in atomic percent. Source: Ref 13.2 Fig. 13.6 Comparison of calculated liquidus, solidus, and γ′ solvus temperatures...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740103
EISBN: 978-1-62708-308-9
... Bulk deformation processes. Source: Ref 1 Fig. 2 Recrystallization during hot rolling. Source: Ref 2 Fig. 3 Relative workabilities of wrought and cast metals. Source: Ref 3 Fig. 10 Open-die forging. Source: Ref 9 Definition Open-die forging is a hot forging...