Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 1998
DOI: 10.31399/asm.tb.ts5.t65900305
EISBN: 978-1-62708-358-4
..., and boride coatings that improve the performance of hot-work and high-speed tool steels. boride coatings chemical vapor deposition electron beam surface modification high-speed tool steel hot-work tool steel ion implantation laser beam surface modification nitriding oxide coatings physical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2022
DOI: 10.31399/asm.tb.dsktmse.t56050001
EISBN: 978-1-62708-432-1
.... It discusses the mechanisms behind interstitial, substitutional, grain boundary, and surface diffusion, the derivation and use of Fick’s laws, and the basic principles of diffusion coating processes, including carburizing, nitriding, nitrocarburizing, cyaniding, carbonitriding, boriding, aluminizing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Fig. 14 Compares the abrasion resistance of TiN coatings applied by various thin-film processes Fig. 15 Compares the surface hardness of hardened tool steel and a cemented carbide with that of the following surface-hardening processes: TRD, CVD, PVD, boriding, chrome plating, electroless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
... Abstract This chapter provides practical information on surface treatments that work by altering the surface chemistry of metals and alloys. It discusses the use of phosphate and chromate conversion coatings as well as anodizing, steam oxidation, diffusion coatings, and pack cementation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280025
EISBN: 978-1-62708-267-9
... in most cobalt-base alloys. Some carbide- and γ′-forming elements may contribute significantly to chemical properties as well. Borides may form in the iron-nickel-and nickel-base superalloys. Detrimental phases also form in the superalloys. Among these phases are σ, μ, and Laves. These phases are so...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2022
DOI: 10.31399/asm.tb.dsktmse.9781627084321
EISBN: 978-1-62708-432-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000111
EISBN: 978-1-62708-313-3
... forms rapidly and is highly adherent to the substrate. Therefore, both chromium and aluminum levels are instrumental in protecting the superalloy. Because the aluminum level in many alloys is insufficient to provide long-term protection, additional protective coatings are often applied. These coatings...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240563
EISBN: 978-1-62708-251-8
..., and secondary fabrication processes. It also covers coating technology, including aluminide diffusion and overlay coatings, and addresses the advantages and disadvantages of superalloys in various applications. cast nickel-based superalloys wrought nickel alloys wrought cobalt-based superalloys cast...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280357
EISBN: 978-1-62708-267-9
... electron vacancy number of particular element n = number of elements in the matrix There was clearly a need in this type of calculation system to incorporate the effects of carbides, borides, and γ′ formation on the γ matrix composition from which the tcp is presumed to form. A plethora...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.t56060001
EISBN: 978-1-62708-440-6
... Abstract This chapter presents the theory and practice associated with the application of thin films. The first half of the chapter describes physical deposition processes in which functional coatings are deposited on component surfaces using mechanical, electromechanical, or thermodynamic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
...) siliconizing Improved oxidation resistance Boronizing (boriding) Improved wear resistance, oxidative wear, and surface fatigue Ion implantation Improved friction and wear resistance for a variety of substrates Laser alloying Improved wear resistance Adding a surface layer or coating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230117
EISBN: 978-1-62708-298-3
... Abstract This chapter discusses the synthesis of important beryllium compounds, including beryllium borides, beryllium carbide, beryllium carbonates, beryllium carboxylates, beryllium halides, beryllium hydride, beryllium hydroxide, beryllium nitrate, beryllium nitride, beryllium oxalate...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.9781627084406
EISBN: 978-1-62708-440-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... with abrasive wear. alclad. Composite wrought product composed of an aluminum alloy core having one or both surfaces a metallurgically bonded aluminum or alu- minum alloy coating that is anodic to the core and thus electrochemi- cally protects the core against corrosion. alkaline cleaner. A material blended...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490265
EISBN: 978-1-62708-340-9
... corrosion assistance Retire; weld repair Need to develop materials with improved pitting resistance; improve design to minimize stress concentration; reduce da/dn; coatings HP/IP rotor Radial-axial bore cracks Creep with or without low-cycle fatigue; poor creep ductility due to faulty heat treatment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
...-aluminum composites and the use of protective coatings and design criteria for corrosion prevention. aluminum-matrix composites coatings corrosion design criteria stress corrosion cracking METAL-MATRIX COMPOSITES (MMCs) are a class of materials with potential for a wide variety of structural...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
... phase and geometrically and topologically close-packed phases, and describes how superalloy microstructure can be modified via heat treatments and directional solidification. It also discusses the role of carbides, borides, oxides, and nitrides and the detrimental effects of sulfocarbides...