1-20 of 463 Search Results for

binder

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290035
EISBN: 978-1-62708-319-5
... Abstract Generally, binders consist of at least three ingredients: a backbone to provide strength (compounds such as polyethylene, polypropylene, ethylene vinyl acetate, and polystyrene); a filler, such as polyacetal and paraffin wax, to occupy space between particles; and additives...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290067
EISBN: 978-1-62708-319-5
... Abstract This chapter provides details on several specific binder formulations and a discussion of basic binder design concepts. The focus is on customization of the feedstock response to heating, pressurization, or solvent exposure for a specific shaping process. The discussion starts...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290085
EISBN: 978-1-62708-319-5
... Abstract This chapter is a detailed account of various attributes related to mixing and testing of powder-binder feedstocks. Mixing parameters and their effects on feedstock properties is discussed. The attributes reviewed include mixture homogeneity, wetting, powder-binder ratio, feedstock...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290139
EISBN: 978-1-62708-319-5
... Abstract Binder removal approaches involve various combinations of heat, solvents, vacuum, and pressure. In each variant, the goal is binder removal without component damage. This chapter addresses the factors that control success, showing how process decisions depend on the powder and binder...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... Abstract This chapter provides details on powder-binder processing for three materials, namely precipitation-hardened 17-4 PH stainless steel, cemented carbides, and alumina. The types of powders, binders, feedstock, shaping processes, debinding, sintering cycles, compositions, microstructure...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290251
EISBN: 978-1-62708-319-5
... Abstract This chapter is intended to identify materials, processes, and designs that will lead to great advances in powder-binder forming technologies. It discusses some of the structures obtained through these advances in powder-binder technologies such as binder jetting and extrusion-based...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Image
Published: 01 August 2013
Fig. 12.14 Sheet metal forming system showing the location of the binder. F b , binder force; F p , punch force; F r , restraining force. Source: Ref 12.7 More
Image
Published: 01 March 2002
Fig. 7.30 Epoxy mounts with binder clips to hold the specimen perpendicular to the polished surface More
Image
Published: 01 August 2013
Fig. 12.13 Binder force profile in a shape-set process to reduce springback in U-channels More
Image
Published: 01 August 2013
Fig. 12.15 Forming problems caused by inadequate binder control. Source: Ref 12.7 More
Image
Published: 01 August 2013
Fig. 15.3 Sheet metal forming system showing the location of the blankholder (binder). Source: Ref 15.2 More
Image
Published: 01 August 2013
Fig. 15.8 Representative binder force trajectories and their effect on sheet forming More
Image
Published: 01 August 2013
Fig. 15.10 Binder force travel trajectories. Source: Ref 15.7 More
Image
Published: 01 August 2013
Fig. 15.11 Effect of binder force trajectory on springback of DP 590 steel. Source: Ref 15.7 More
Image
Published: 01 August 2013
Fig. 15.12 Multipoint active binder. Photo courtesy of Muller-Weingarten More
Image
Published: 01 August 2013
Fig. 15.13 Rigid binder with nitrogen cylinders. Courtesy of TDM/Ford Motor Co. More
Image
Published: 01 August 2013
Fig. 15.14 Schematic of a flexible binder system with hydraulic cylinders. Source: Ref 15.9 More
Image
Published: 01 August 2013
Fig. 15.15 Basic components of a flexible binder control unit. Source: Ref 15.4 More
Image
Published: 01 August 2013
Fig. 15.16 Real-time process control system for flexible binder. Source: Ref 15.9 More