Skip Nav Destination
Close Modal
Search Results for
bimetal plate
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-14 of 14 Search Results for
bimetal plate
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170528
EISBN: 978-1-62708-297-6
...-acid storage batteries (in the grid plates, posts, and connector straps), ammunition, cable sheathing, and building construction materials (such as sheet, pipe, solder, and wool for caulking). Other important applications include counterweights, battery clamps and other cast products such as: bearings...
Abstract
This article examines the role of alloying in the production and use of lead and tin. It describes the various categories and grades of lead and lead-base alloys along with their nominal compositions and corresponding UNS numbers. It also discusses the composition and properties of lead used in battery grids, type metals, and bearings. It, likewise, discusses the use of tin in various types of solder and in bearings and provides composition and property data for application-specific designations and grades. The article also discusses the effect of impurities in tin-lead solders and the amounts and combinations in which they are found.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Abstract
This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic coatings and various pack cementation and deposition processes. It also discusses the selection and use of industrial paints and paint application methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
... are typically less than for wrought products. Tooling can range from simple patterns to complex tool steel dies depending on product requirements and production volume. Metallurgically or mechanically bonded bimetal parts can be routinely cast. Aluminum parts are routinely cast by every known process...
Abstract
This chapter first introduces the various factors that may alter the physical and mechanical properties of aluminum castings that are addressed in the other chapters in the book. Then, it presents the historical development of aluminum castings, followed by a discussion on the advantages and limitations of aluminum castings. Next, the chapter describes the major trends that are influencing the increased use of aluminum castings. Finally, it introduces the considerations involved in the selection of an appropriate aluminum alloy and casting process for a given application.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500001
EISBN: 978-1-62708-317-1
... Influence of lubrication on punch wear. Source: Ref 1.9 Stripper Plate <xref rid="t53500001-ref3" ref-type="bibr">(Ref 1.3)</xref> Stripper plate plays three important roles in blanking: The part is held firmly during the blanking operation by the stripper. The punch is guided...
Abstract
This chapter provides an overview of the blanking process and the forces and stresses involved. It discusses the factors that affect part quality and tool life, including punch and die geometry, stagger, clearance, and wear as well as punch velocities, misalignment, and snap-thru forces. It also discusses ultra-high-speed blanking, fine blanking, and shearing, and the use finite-element simulations to predict part edge quality.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230163
EISBN: 978-1-62708-298-3
... plates, and hot rolled to approximately 50% reduction. The material was then annealed, rejacketed, and rerolled as necessary to produce the final thickness of plate or sheet material required [ London 1979 ]. Extrusion and rolling were conducted in the 510 to 565 °C (950 to 1050 °F) range. Both...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200437
EISBN: 978-1-62708-354-6
... plate A second bottom board on which molds are opened. Bainite . . . In steel, an acicular aggregate of ferrite and carbide, resulting from an isothermal transformation of austenite at a temperature below the pearlitic range and above Ms. Baked Core . . . A core which has been heated for a sufficient...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400169
EISBN: 978-1-62708-258-7
... oxide particles can be retained in voids in the specimen or at the specimen surface (at a steel/oxide-scale interface or a steel/mounting material interface, etc.). Figure 7.1 shows an example of silicon carbide particles embedded into the polished surface of a nickel-plated steel specimen...
Abstract
This chapter instructs the metallographer on the basic skills required to prepare a polished metallographic specimen. It is organized in a chronological sequence starting with the information-gathering process on the material being investigated, then moving on to sectioning, mounting, grinding, and polishing processes, and ending with methods used to properly store metallographic specimens. The discussion covers the preparation procedures, the materials being investigated, and equipment used to perform these procedures.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
Abstract
Nonferrous metals are of commercial interest both as engineering materials and as alloying agents. This chapter addresses both roles, discussing the properties, processing characteristics, and applications of several categories of nonferrous metals, including light metals, corrosion-resistance alloys, superalloys, refractory metals, low-melting-point metals, reactive metals, precious metals, rare earth metals, and metalloids or semimetals. It also provides a brief summary on special-purpose materials, including uranium, vanadium, magnetic alloys, and thermocouple materials.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540047
EISBN: 978-1-62708-309-6
... with compression tests is the application of compression loads to a thin plate having a rectangular cross section. Although some special jigs are available for this purpose, it is almost impossible to obtain a compression stress-strain curve for a thin plate by taking a simple compression test. However...
Abstract
This chapter examines the phenomena of deformation and fracture in metals, providing readers with an understanding of why it occurs and how it can be prevented. It begins with a detailed review of tension and compression stress-strain curves, explaining how they are produced and what they reveal about the load-carrying characteristics of engineering materials. It then discusses the use of failure criteria and the determination of yielding and fracture limits. It goes on to describe the mechanisms and appearances of brittle and ductile fractures and stress rupture, providing detailed images, diagrams, and explanations. It discusses the various factors that influence strength and ductility, including grain size, loading rate, and temperature. It also provides information on the origin of residual stresses, the concept of toughness, and the damage mechanisms associated with creep and stress rupture, stress corrosion, and hydrogen embrittlement.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
.... , 1975 . “ Beryllium/Titanium Bimetal System ,” Naval Air System Command Contract: N00019–74-C-0017, Report AD-A-019657, Pratt and Whitney Aircraft Division, United Technologies Company CRC , 1971–1972 . Handbook of Chemistry and Physics , The Chemical Rubber Company Press , Cleveland, OH...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3