1-20 of 148 Search Results for

beryllium-nickel alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By Kenneth A. Walsh
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230001
EISBN: 978-1-62708-298-3
...Abstract Abstract Beryllium, despite its relatively simple atomic structure, possesses a wide range of useful engineering properties. It has the highest strength-to-weight ratio and modulus of elasticity among structural metals and is an important alloy addition in copper, nickel, and aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240135
EISBN: 978-1-62708-251-8
...Abstract Abstract Precipitation hardening is used extensively to strengthen aluminum alloys, magnesium alloys, nickel-base superalloys, beryllium-copper alloys, and precipitation-hardening stainless steels. This chapter discusses two types of particle strengthening: precipitation hardening...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240469
EISBN: 978-1-62708-251-8
..., and corrosion resistance. This chapter covers the classification, composition, properties, and applications of copper alloys, including brasses, bronzes, copper-nickel, beryllium-copper, and casting alloys. It also examines wrought copper alloys and pure coppers. The chapter begins with an overview...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
... erosion. It also discusses the tribology of nickel- and cobalt-base alloys as well as titanium, zinc, tin, aluminum, magnesium, beryllium, graphite, and different types of wood. References References 1. Hanson J. S. , The Relative Erosion Resistance of Several Materials , Erosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850509
EISBN: 978-1-62708-260-0
...Abstract Abstract This appendix provides a list of etch compositions and procedures that reveal the macrostructure of aluminum, beryllium, bismuth, antimony, cobalt, copper, lead, magnesium, nickel, tin, titanium, zinc, and their respective alloys as well as iron, steel, noble metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230179
EISBN: 978-1-62708-298-3
... Okamoto H. , Tanner L.E. , and Peterson D.E. , 1991 . Beryllium-Nickel Phase Diagram , Phase Diagrams of Binary Nickel Alloys , ASM International Okamoto H. , Tanner L.E. , and Peterson D.E. , 1993 . Iron-Beryllium Phase Diagram , Phase Diagrams of Binary Iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240597
EISBN: 978-1-62708-251-8
...Abstract Abstract This chapter discusses the compositions, properties, and applications of nonferrous metals, including zirconium, hafnium, beryllium, lead, tin, gold, silver, and platinum group metals. It also addresses fusible alloys and provides melting temperatures for several compositions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440231
EISBN: 978-1-62708-262-4
... structures Copper-base alloys Beryllium bronze (beryllium copper) 1.9 Be, 0.2 Co or Ni Surgical instruments, electrical contacts, nonsparking tools, springs, nuts, gears, and other heavy duty applications Aluminum bronze 10 Al, 1 Fe Applications requiring resistance to corrosion, stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230007
EISBN: 978-1-62708-298-3
... importance emerged from the developmental programs with the discovery of the exceptional mechanical properties of metals alloyed with beryllium. The ability of beryllium, with the addition of small amounts of nickel, to age harden copper was discovered by Corson in 1926. Michael G. Corson was a metallurgist...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... that of aluminum, and more than six times that of magnesium. The modulus of beryllium is also approximately one and a half times the modulus of most iron and nickel alloys. In addition to the applications of beryllium as a base material, it is also used as an alloy addition to copper to produce a high-strength...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170457
EISBN: 978-1-62708-297-6
... elements are often present in copper and its alloys. As a result, the requirement of an effective ventilation system to protect the welder and/or the welding machine operator is more critical than when welding ferrous metals. Zinc Tin Beryllium, Aluminum, and Nickel Silicon Phosphorus...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230163
EISBN: 978-1-62708-298-3
... elements form substantive solid solutions in beryllium metal, that is, copper, nickel, cobalt, and, to a lesser extent, iron. Silver has limited solid solubility in beryllium. Most solid-solution alloys are substantially stronger than the purified metal, that is, metal from which microalloying-type...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
.... Pure coppers have good ductility (up to 50% elongation) as do some brasses, monels, and some copper-nickel-zinc alloys. Some of the bronzes and other alloys in cast form have elongations that may be less than 10%. The tensile strengths can range from about 1700 MPa (247,000 psi) for beryllium copper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230493
EISBN: 978-1-62708-298-3
... described previously. If the beryllium oxide ceramic is metallized (molybdenum, manganese, nickel, and copper), the metals must be chemically milled before recycling. The beryllium oxide is then crushed and recycled to the arc furnace. A dross processing operation separates true dross components from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230151
EISBN: 978-1-62708-298-3
..., “Beryllium Intermetallic Compounds,” in this book. Beryllium is an important alloying addition to copper and nickel, where it provides for a precipitation-hardenable alloy. It is also useful for the control of aluminum melting and casting because of its strong affinity for oxygen. The alpha phase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230401
EISBN: 978-1-62708-298-3
... by soldering. By first plating beryllium with copper and then nickel, beryllium surfaces can be joined to each other using silver solder [ Jacobson 1986 ]. Beryllium has been successfully welded by several processes, including gas tungsten arc and electron beam welding. The welding operations should...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... steel 7.6–15 4.2–8.5 Pure Scandium (Sc) 11–12 6.1–6.8 Pure Beryllium (Be) 6.3–17 3.5–9.4 Carbide 10–13 5.7–7.3 Nickel chromium molybdenum alloy steel 11–12 6.1–6.9 Shock-resisting tool steel 12 6.5 Structural steel 11–13 5.9–7.1 Air hardening medium-alloy cold work...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230131
EISBN: 978-1-62708-298-3
... A.J. , and Walsh K.A. , 1970 . Micro-Alloying Relationships in Beryllium , Proc. Beryllium Conf. , National Academy of Sciences , Washington, D.C. , p 127 – 147 Hanrahan R.J. Jr. , Thoma D.J. , Jacobson L.A. , Zocco T.G. , Lowery J.L. , and Pereyra R...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... Spectroscopy (SIMS 7) ( Chichester, U.K. ), Wiley, p 727 – 730 Roybal E.A. , McIntosh M.B. , and Hull H.K. , 1997 . Current Status of Optical Grade Sputtered, Bare Beryllium, and Nickel-Plated Beryllium , Critical Reviews of Optical Science and Technology, Advanced Materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230145
EISBN: 978-1-62708-298-3
... performed by the same group reported on the investigation of the influence of beryllium on the thermal stability of the Zr-Al-Ni-Cu bulk amorphous alloys [ Xiao et al. 2004 ]. With the aluminum, nickel, and copper held at constant atomic percentages of 10, 10, and 15, respectively, the zirconium composition...