Published: 01 July 2009
Fig. 6.4 Tall oil fatty acid flotation of phenacite and bertrandite. Source: Bulatovic 1988 More
Image
Published: 01 July 2009
Fig. 7.2 Beryllium extraction from beryl and bertrandite ores at the Delta Plant in Utah by Brush Resources, Inc. Note: CCD thickeners are used in the countercurrent decantation (CCD) process to separate sludge and concentrate from solution. More
Book Chapter

By Edgar E. Vidal, James Foley, David L. Olson
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230065
EISBN: 978-1-62708-298-3
... Abstract This chapter describes some of the processes used to concentrate beryllium-rich minerals from ores. It discusses the flotation of bertrandite and phenacite from calcite, mica, fluorspar, and quartz-containing ores, the flotation of beryl from pegmatitic gangues and low-grade deposits...
Book Chapter

By Kenneth A. Walsh, Edgar E. Vidal
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230019
EISBN: 978-1-62708-298-3
... Abstract Beryllium is the 44th most abundant element on Earth, with an estimated concentration of six parts per million in the Earth’s crust. It is found in various forms in more than 100 minerals, two of which, beryl and bertrandite, account for most of the beryllium produced throughout...
Book Chapter

By Kenneth A. Walsh, Edgar E. Vidal, Brajendra Mishra
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230071
EISBN: 978-1-62708-298-3
... of the briquettes was promoted by the sodium carbonate addition. The beryllium hydroxide product recovered 85 wt% of the beryllium content of the ore. 7.5 Extraction from Bertrandite and Solvent Extraction The volcanic tuff beds in the Topaz-Spor Mountain, Utah, are a source of beryllium that contains only...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230007
EISBN: 978-1-62708-298-3
... bertrandite. A large volume of information on beryllium was published jointly in 1975 by the USSR Academy of Sciences and the USSR Ministry of Geology [ Kogan et al 1975 ]. This book contains extensive descriptions of worldwide distribution of beryllium-containing ores, applications of beryllium gleaned...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230093
EISBN: 978-1-62708-298-3
... important beryllium compound. It is the product of the extraction processes used for beryl, helvite, and bertrandite ores. This beryllium hydroxide has variable degrees of purity. It becomes the intermediate for the production of metallic beryllium, ceramic-grade beryllium oxide, and beryllium-containing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3