Fig. 4.15 Modern Hazelett model AS2000 twin-belt caster. Courtesy of Hazelett Strip Casting Corp. More
Image
Published: 30 June 2023
Fig. 4.16 Process flow for typical Hazelett twin-belt caster production. More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340063
EISBN: 978-1-62708-427-7
..., molten metal treatment, control of inclusions, ingot grain refinement, and direct chill (DC) or continuous casting. aluminum alloys belt casters continuous casting direct chill ingot casting inclusions melting molten metal processing scrap charging Direct chill (DC) ingots used...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370021
EISBN: 978-1-62708-447-5
... of the mulled or prepared sand at room temperature. The sand mix is discharged into a chute, and a short belt conveyor delivers the sand mix to a bucket elevator, which discharges the sand mix onto a belt conveyor with an over-the-belt aerator. The aerator breaks up the sand lumps, making the sand mix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310225
EISBN: 978-1-62708-286-0
... of stainless steel. Exhaust systems constitute the largest use of stainless steel in the automotive market, but there are other important applications that cannot be ignored: valves and gaskets, hose clamps, seat belt and air bag components, tubing, hardware, and filters. And, there will be new...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340339
EISBN: 978-1-62708-427-7
... during lamination. Manganese, chromium, and other impurities are carefully limited to control strength and grain size. Converter foil can be produced from twin-roll casters, slab casters, or the traditional DC ingot/hot-roll path, as discussed in Chapters 4 and 6 . In the United States, 80–90...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410103
EISBN: 978-1-62708-280-8
... and sheared off or trimmed in a trim press, using trim dies. The parting line at the gate should be chosen to ensure that the trimmed edges can be belt sanded to remove burrs. Circular or tubular sections may need a thin pad along the parting line to ensure that the trimmed edge does not damage the casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200206
EISBN: 978-1-62708-354-6
... grinding (e.g., belt sanding grinding or surface grinding to gage) 3.2 Hand straighten to gage 3.3 Hydraulic press to gage 3.4 Coining to gage (a) 3.5 Machine locating points (a) 3.6 Rough machine to gage (a) 3.7 Target machine casting (a) 3.8 Finish machine part...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
... system or casting cavity to form oxides. Metal casters use computer analysis of gating systems to indicate when reoxidation can be expected in a gating system and to eliminate it. However, casting designs that require molten metal to “jet” through a section of the casting to fill other sections...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240349
EISBN: 978-1-62708-251-8
... melting and slag formation. (Slag floats on top of the molten iron and absorbs many of the unwanted impurities.) Fine ore is mixed with the coke and fluxes and heated in a sinter plant on a continuous moving belt on which the coke is ignited. The high temperatures generated fuse the ore particles...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
...-quality castings. The strainer cores are made from high-strength core mixes (with iron oxide). They are set in the pouring cup either at the top of the sprue, as shown in Fig. 7.13(a) , or at the bottom of the sprue (to act as a choke), as shown in Fig. 7.13(b) . Some casters use strainer cores made...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
... of the unwanted impurities. Fine ore is mixed with the coke and fluxes and heated in a sinter plant on a continuous moving belt on which the coke is ignited. The high temperatures generated fuse the ore particles and fluxes together to form a porous clinker called sinter. The use of sinter in the blast furnace...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9