Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110196
EISBN: 978-1-62708-247-1
..., junctions, and complete devices. The article also provides a description and case study examples of multiple photocurrent and thermal injection techniques. The photocurrent examples are based on Optical Beam-Induced Current and Light-Induced Voltage Alteration. The thermal stimulus examples are Optical Beam...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
...Abstract Abstract Nickel and nickel-base alloys are specified for many applications, such as oil and gas production, power generation, and chemical processing, because of their resistance to stress-corrosion cracking (SCC). Under certain conditions, however, SCC can be a concern. This chapter...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110180
EISBN: 978-1-62708-247-1
... mechanisms of PE in silicon based ICs. It presents the opportunities of contactless characterization for the most important electronic device, the MOS - Field Effect Transistor, the heart of ICs and their basic digital element, the CMOS inverter. The article discusses the specification and selection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270185
EISBN: 978-1-62708-301-0
... optical and electron microscopes, indicating that the operating loads on the bolts far exceeded the design loads. Based on their observations, which are summarized in the report, failure analysts concluded that the design of the connecting rod system needs to be reassessed. connecting rod bolts SEM...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850533
EISBN: 978-1-62708-260-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060111
EISBN: 978-1-62708-343-0
... 871 1600 0.2 0.87 0.21 1.08 1234 179 214 871 1600 0.2 0.43 0.01 0.44 616 89 17,731 Flow and failure constants for total strain version of strain-range partitioning characterization of nickel-base superalloy B-1900+Hf out-of-phase bithermal results 483 ⇔ 871 °C (900 ⇔ 1600 °F...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490183
EISBN: 978-1-62708-340-9
... thickness; y is metal loss (penetration); T is temperature; t is time, in hours; all logarithms to base 10. °R = °F + 460; K = °C + 273; 1 mm = 10 3 μm = 40 mils; y = 0.42x. General forms of the oxide correlations for Cr-Mo steels (<xref ref-type="bibr" rid="t60490183-ref52">Ref 52</xref>) Table...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000009
EISBN: 978-1-62708-313-3
...Abstract Abstract This chapter provides a brief overview of nickel-iron-base, cobalt-base, and nickel-base superalloys, discussing their basic metallurgy and defining characteristics. coefficient of thermal expansion superalloys SUPERALLOYS ARE CLASSIFIED according to the main...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
...Abstract Abstract This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170003
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the general purpose of alloying and identifies some of the material properties and behaviors that can be improved by adding various elements to the base metal. It explains how alloying can make metals stronger and more resistant to corrosion and wear...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130001
EISBN: 978-1-62708-284-6
...Abstract Abstract A systematic procedure for minimizing risks involved in heat treated steel components requires a combination of metallurgical failure analysis and fitness for service with respect to safety and reliability based on risk analysis. This chapter begins with an overview of heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270067
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed in service, causing extensive engine damage. A section of the blade broke off around 25 mm from the root platform, producing a flat fracture surface that appeared smooth on one end and grainy elsewhere. Based on their examination...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270126
EISBN: 978-1-62708-301-0
...Abstract Abstract A test flight was cut short after a fire warning came on indicating a problem with one of the four engines on an aircraft. A visual examination following the precautionary landing revealed several burned hoses, a melted bolt, and fuel leaking from the base of the main burner...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270143
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed during a test run, causing extensive damage to an aircraft engine. Visual examination showed that the nickel-base superalloy blade broke above the root platform in the airfoil section, leaving a fracture surface with two distinct...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270182
EISBN: 978-1-62708-301-0
...Abstract Abstract A turbine in a fertilizer plant began to vibrate and was shut down to investigate the problem. A first stage rotor blade was found fractured and was removed along with several other blades for further examination. Based on their observations and testing, investigators...