1-20 of 765 Search Results for

base materials selection

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170123
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the role of alloying in the production and use of carbon and low-alloy steels. It explains how steels are defined and selected based on alloy content and provides composition and property data for a wide range of designations and grades. It describes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
.... The testing of filament-wound composite materials offers unique challenges because of the special characteristics of composites. This chapter describes suitable static mechanical test techniques for characterizing laminated composite materials. The approach is to provide recommended techniques, based...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060369
EISBN: 978-1-62708-261-7
... or salts of the base material. This chapter discusses the process of corrosion and how to prevent or mitigate its effects. It describes several forms of corrosion, including uniform, intergranular, pitting, crevice, and stray-current corrosion, and the effects of stress-corrosion cracking, corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
..., and appearance of the corroded metal. It discusses five primary methods of corrosion control, namely, material selection, coatings, inhibitors, cathodic protection, and design. Examples of the opportunities in corrosion control and the means to implement a program to capitalize on those opportunities...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
...Abstract Abstract This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms. It includes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030247
EISBN: 978-1-62708-282-2
...). f r = V t − V s g h eff Summary: Corrosion rate in fully developed turbulent pipe flows computed from field conditions of vertical or horizontal flow can be understood based on selected flow modeling parameters. Corrosion under field conditions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700215
EISBN: 978-1-62708-279-2
... for materials selection. forming welding advanced high-strength steels car body structures performance indices THE INCREASED USE OF advanced high-strength steels (AHSS) has created a need to develop a knowledge base of data and experiences aimed at the successful applications of the new materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820001
EISBN: 978-1-62708-339-3
... to Environments Containing Hydrogen Sulfide Microbiologically Influenced Corrosion (MIC) Heat-Tint Oxide Formation Material and Welding Consumable Selection Surface Preparation Welding Design Welding Practice Weld Surface Finishing Surface Coating Postweld Heat Treatment Preheat...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780055
EISBN: 978-1-62708-281-5
..., 103.4 MPa (15 ksi) Fig. 13 Design-based material-selection process Fig. 14 Geometry of enclosure example Fig. 12 In-mold cooling time versus wall thickness predicted from one-dimensional, transient mold cooling analysis Material Unfilled PC Thickness, mm 1.62...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... Maintainability Specification coverage Availability of design data Experience base with this or similar materials Selection considerations Expected total life or plant or process Estimated service life of material Reliability (safety and economic consequences of failure) Availability...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820169
EISBN: 978-1-62708-339-3
.... A36 structural steel was selected as the base metal. The chemical compositions of these materials are listed in Table 1 . The results of this study demonstrated that hydrogen introduced during welding can lead to hydrogen-induced cracking in dissimilar welds between austenitic filler metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820143
EISBN: 978-1-62708-339-3
...) Maximum Relative rating of selected aluminum filler alloys used to fillet weld or butt weld two component base alloys, where one of the base alloys is 319.0, 333.0, 354.0, 355.0, C355.0, or 380.0 Table 3(a) Relative rating of selected aluminum filler alloys used to fillet weld or butt weld two...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
.... (c) Balance—remaining percentage is made up of lead. Source: Ref 7.1 Tin-Lead Solders Lead-Free Solders Other Solder Alloys A sound soldered joint is achieved by selecting and using the proper materials and processes. Base metals are usually selected to achieve the specific...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040277
EISBN: 978-1-62708-300-3
... (800 °C) Very high Very high Laser High Same as base High High PFS High Tailorable Not applicable High to very high Properties of materials that determine their selection as die materials for hot forging are: Ability to harden uniformly Wear resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
...Abstract Abstract Joining comprises a large number of processes used to assemble individual parts into a larger, more complex component or assembly. The selection of an appropriate design to join parts is based on several considerations related to both the product and the joining process. Many...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280365
EISBN: 978-1-62708-267-9
.... , ASM International , 1999 , p 394 – 414 10.31399/asm.hb.mhde2.a0003120 • Furrer D. and Fecht H. , Ni-Base Superalloys for Turbine Disks , J. Met. , Vol 51 ( No. 1 ), 1999 , p 14 – 17 10.1007/s11837-999-0005-y • Davis J.R. , Ed., Heat-Resistant Materials , ASM...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... , Engineered Materials Handbook Desk Edition , ASM International , 1995 10.31399/asm.hb.emde.a0003065 10.7 Joining Ceramics , Engineered Materials Handbook Desk Edition , ASM International , 1995 10.31399/asm.hb.emde.a0003056 Selected References Selected References • DuPont J.N...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000001
EISBN: 978-1-62708-313-3
... States had developed its first aircraft GTE in 1943, cobalt-base superalloys had been introduced, and Haynes Stellite 21 (a cast alloy intended primarily for dental implants) was chosen as the very first turbine blade material. Most of the early nickel-iron- and cobalt-base alloys were strengthened...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040257
EISBN: 978-1-62708-300-3
... material is extremely crucial for the design of an isothermal forging process, since the selection of the other elements, such as equipment, die material, and lubricants, is based on this knowledge. At hot forging temperatures (T ≥ T m , where T m is the melting point or solidus temperature...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870161
EISBN: 978-1-62708-299-0
.... Fig. 1 Effect of the heat of welding on microstructure, hardness, and corrosion potential of welded assemblies of three aluminum alloys. The differences in corrosion potential between the heat-affected zone (HAZ) and the base metal can lead to selective corrosion. (a) Alloy 5456-H321 base metal...