1-20 of 502 Search Results for

bar

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480225
EISBN: 978-1-62708-318-8
... to convert titanium billet and bar into useful shapes or more refined product forms. These secondary working operations include open-die, closed-die, hot-die and isothermal forging as well as ring rolling and extruding. The chapter describes each method in detail and how it affects the microstructure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720321
EISBN: 978-1-62708-305-8
... of probe, rev/min 1000 Signal transmit Noncontact rotation transmit Marker One each for near-surface flaw and inside flaw Source: Ref 2 Specifications of an ultrasonic flaw detection system for cold drawn hexagonal bars Table 2 Specifications of an ultrasonic flaw detection system...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220519
EISBN: 978-1-62708-259-4
..., quenched and tempered, bainitic structure. Hardness 240 HB. Courtesy of A. Zeemann, Tecmetal, RJ, Brazil. Abstract Abstract This chapter examines the microstructure of special bar quality (or engineering) steels and how it is influenced by carbon content, tempering temperature, and prior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040141
EISBN: 978-1-62708-300-3
... . The transverse rolling machines are suitable for automatic production, using bar stock automatically fed to the rolls through an induction heating unit. Fig. 12.7 Principle of operation of transverse rolling machines. [ Neuberger et al., 1968 ] Fig. 12.8 Forging produced in a transverse rolling...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040151
EISBN: 978-1-62708-300-3
... C. , Vasquez V. , Altan T. , “ Simulation of Bar Shearing Process, ” ERC/NSM-97-27, Engineering Research Center for Net Shape Manufacturing . [Duvari et al., 2003] Duvari S. , Isbir S. , Ngaile G. , Altan T. , “ Optimization of Tool Design in Hot Shearing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130311
EISBN: 978-1-62708-284-6
... regions, which are the working areas of die-casting dies (Ref 32) . Fig. 36 Charpy V-notch (CVN) results for different heat treating conditions of H13 tool steel, carried out at room temperature and at 425 °C. Specimens cooled at various rates, simulating the core of 150 and 300 mm round bars...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410197
EISBN: 978-1-62708-265-5
... treating eutectoid, hypoeutectoid, and proeutectoid steels. It also provides references to large collections of transformation diagrams and includes several diagrams that plot quenching and hardening transformations as a function of bar diameter. continuous cooling transformation diagram isothermal...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240221
EISBN: 978-1-62708-251-8
... and causes of these failure modes. Some body-centered cubic and hexagonal close-packed metals, and steels in particular, exhibit a ductile-to-brittle transition when loaded under impact and the chapter describes the use of notched bar impact testing to determine the temperature at which a normally ductile...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120327
EISBN: 978-1-62708-269-3
... on density of 0.163 lb/in. 3 . s, sheet; p, plate. Courtesy of Supra Alloys, Inc. Titanium flat bar weights Table H.2 Titanium flat bar weights Weight, lb/ft, at width (in.): Thickness, in. ½ ⅝ ¾ ⅞ 1 1¼ 1½ 1¾ 2 2¼ 2½ 2¾ 3 3¼ 3½ 3¾ 4 ¼ 0.244 0.305 0.366 0.427 0.488...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220009
EISBN: 978-1-62708-341-6
.... The chapter reviews the mechanistic basis for induction heating and provides an example of eddy-current distribution in a solid bar. The chapter defines two important concepts in the technology of induction heating: equivalent resistance and electrical efficiency. The chapter concludes with a discussion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220253
EISBN: 978-1-62708-341-6
... billet heating, bar heating, heat treatment, soldering, brazing, and other induction-based processes. The final section discusses the use of robots for parts handling in induction heating systems. automation induction bar heating induction billet heating induction brazing induction heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
...Abstract Abstract The hot-working process extrusion is used to produce semifinished products in the form of bar, strip, and solid sections, as well as tubes and hollow sections. The first part of this chapter describes the composition, properties, and applications of tin and lead extruded...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870157
EISBN: 978-1-62708-344-7
... of flexural bending on solid as well as hollow rectangular and round bars. The chapter also discusses the difference in the treatment of a rotating shaft in which all surface elements undergo the same stress and strain and a nonrotating shaft in which a few surface elements carry most of the load...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
...Abstract Abstract This chapter presents various case histories that illustrate a variety of failure mechanisms experienced by the high-strength steel components in aerospace applications. The components covered are catapult holdback bar, AISI 420 stainless steel roll pin, main landing gear (MLG...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310213
EISBN: 978-1-62708-286-0
..., flatness, maintenance, repair, fabrication, and service considerations. It ends with a section providing information on concrete reinforcing bar. References References 1 Stainless Steel Selection Criteria, Contrarian Metal Resources , www.metalresources.net , accessed June 2008 . 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540395
EISBN: 978-1-62708-309-6
...Abstract Abstract This appendix contains figures that illustrate specimen orientation and crack plane codes for rolled plate, drawn bars, and hollow cylinders. drawn bars fracture plane hollow cylinders rolled plate specimen orientation Fig. A6.1 Conventional specimen...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000133
EISBN: 978-1-62708-313-3
...) 21 °C (70 °F) 540 °C (1000 °F) 760 °C (1400 °F) 21 °C 540 °C 760 °C MPa ksi MPa ksi MPa ksi MPa ksi MPa ksi MPa ksi (70 °F) (1000 °F) (1400 °F) Nickel-base Astroloy Bar 1415 205 1240 180 1160 168 1050 152 965 140 910 132 16 16 21 Cabot 214 … 915...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
... strength at 0.2% offset at: Tensile elongation, % at: 21 °C (70 °F) 540 °C (1000 °F) 760 °C (1400 °F) 21 °C (70 °F) 540 °C (1000 °F) 760 °C (1400 °F) 21 °C (70 °F) 540 °C (1000 °F) 760 °C (1400 °F) MPa ksi MPa ksi MPa ksi MPa ksi MPa ksi MPa ksi Nickel-base Astroloy Bar...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140083
EISBN: 978-1-62708-264-8
... confused with hardness, and one intent of this chapter is to distinguish the difference between these two concepts. The general process of hardening a steel (for example, a round bar) involves three steps: Austenitization: The steel is heated to form austenite (usually 100% austenite...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410335
EISBN: 978-1-62708-265-5
... that demonstrates the striking effect of various factors on hardenability is the quenching of series of round bars of various diameters. The bars are completely austenitized, quenched, and tempered. Hardness readings are then taken along diameters of the bar cross sections in order to show the distribution...