1-20 of 128 Search Results for

automotive engine-lubricants

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040237
EISBN: 978-1-62708-300-3
... and the process conditions (i.e., rate of deformation, lubrication, and friction). Other factors that influence fracture include chemical composition, microstructure, surface conditions, and homogeneity. At the Engineering Research Center for Net Shape Manufacturing (ERC/NSM), a methodology for predicting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040319
EISBN: 978-1-62708-300-3
... considerable progress in tooling and equipment design, materials engineering, and lubrication techniques in order to produce precise components. Some of these developments and future trends are discussed in the subsequent sections. Enclosed-die forging uses multiple-action tooling as punches press...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630169
EISBN: 978-1-62708-270-9
... • Erosion, Wear, and Interfaces with Corrosion , ASTM , STP 567, 1974 • Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook , ASM International , 1992 • Peterson M.B. and Winer W.O. , Ed., Wear Control Handbook , American Society of Mechanical Engineers , 1980...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500107
EISBN: 978-1-62708-317-1
... 769 – 785 10.1016/S0749-6419(01)00054-7 6.9 Zhu H. , Huang L. , and Wong C. , “Unloading Modulus on Springback in Steels,” Society of Automotive Engineering , 2004 6.10 Perez R. , Benito A. , and Prado J.M. , Study of the Inelastic Response of TRIP...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400089
EISBN: 978-1-62708-316-4
.... , Schmid S. and Yoshida M. , Environmentally Benign Tribo-systems for Metal Forming , Annals of CIRP , Vol 59 ( No. 2 ), 2010 , p 760 – 780 10.1016/j.cirp.2010.05.007 7.10 Meiler M. and Jachke H. , Lubrication of Aluminium Sheet Metal within Automotive Industry...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040001
EISBN: 978-1-62708-300-3
... are extremely important (e.g., load-carrying aircraft, jet engine, and turbine components). The design, analysis, and optimization of forming processes require: Engineering knowledge regarding metal flow, stresses, and heat transfer Technological information related to lubrication, heating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... Premium engineered casting aircraft pylons Fig. 3.18 Premium engineered casting aircraft wing flap Fig. 3.19 Premium engineered casting aircraft canopy Fig. 3.10 Alloy A356.0 alloy automotive wheels produced by low-pressure casting Fig. 3.11 Variety of parts...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300421
EISBN: 978-1-62708-323-2
... than steel transfer. Tin is corrosion resistant enough to resist chemical attack by foods when used as the protective plating in tin cans. As the basis of Babbitt, it is used in automotive crank bearings and as poured Babbitt bearings for large rotating machines. They are used lubricated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400005
EISBN: 978-1-62708-316-4
... industry (fuel tanks, missile cases, jet engine rings, etc.); automotive industry (wheel rims for cars and trucks, etc.). Fig. 2.29 Expanding. Source: Ref 2.4 Dimpling is a process for producing small conical flanges around holes in sheet metal parts that are to be assembled with flush...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630189
EISBN: 978-1-62708-270-9
.../630050 • Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook , ASM International , 1992 • Littmann W.E. and Moyer C.A. , “ Competitive Modes of Failure in Rolling Contact Fatigue ,” Preprint 620A, Society of Automotive Engineers , 1963 10.4271/630003...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700177
EISBN: 978-1-62708-279-2
...Abstract Abstract This chapter describes the nature of the problems arising from using advanced high-strength steels (AHSS) and discusses potential remedies to minimize the adverse effects that may limit the adoption of AHSS in the automotive industry. The discussion provides information...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... applications of low-pressure permanent molding process Industry Typical products (no sand cores) Typical products (sand cores) Automotive Wheels Knuckles Control arms Cross members Engine blocks Cylinder heads hollow Control arms Differential carriers Cored cross members Truck market...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500083
EISBN: 978-1-62708-317-1
... formability magnesium alloys warm forming ONE OF THE MAJOR GOALS of engineering design and manufacturing is weight reduction to save energy. One way to achieve energy savings without jeopardizing the structural integrity of the product is to use lightweight metals, such as aluminum, magnesium, titanium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500179
EISBN: 978-1-62708-317-1
..., and other household appliances, such as refrigerator handles and so on. Typical automotive parts that are produced using THF include exhaust manifolds, chassis parts, engine cradles, catalytic converters, radiator frames, and shock absorber housings. Figure 9.2 shows examples of parts made by THF...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
.... However, a designer must select a specific grade and a specific mating material. What is the best grade to use for a lubricated reciprocating tribosystem? Gray cast iron versus hard iron or a hard steel has been the gold standard for the internal combustion (IC) engine cylinder and piston ring tribosystem...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
.... , “Tool Materials, Coatings and Lubricants to Reduce Tool Wear in Forming AHSS,” Workshop on Forming of AHSS , 2009 16.3 Rooij M.B.D. and Schipper D.J. , Analysis of Material Transfer from a Soft Workpiece to a Hard Tool, Part II: Experimental Verification of the Proposed Lump Growth...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740373
EISBN: 978-1-62708-308-9
... applications are shown in Fig. 1 . On average across all geographical regions, approximately 80% of all P/M structural components are for automotive applications. Approximately 75% of these automotive applications are components for transmissions (automatic and manual) and for engines. Other important...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
...-94-009-1501-5 • Surface Engineering , Vol 5 , ASM Handbook , ASM International , 1994 10.31399/asm.hb.v05.9781627081702 • Surface Treatments and Coatings for Friction and Wear Control , Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook , ASM International...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
... include: Remove hard, adhesive foreign particles with filters for air, water, and oil . The automotive engine is a good example of this. Air and oil filters are used to prevent the entry of external foreign particles and to trap and collect internal foreign particles before they damage the engine...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400001
EISBN: 978-1-62708-316-4
..., in examples such as load-carrying aircraft and jet engine and turbine components. The design, analysis and optimization of forming processes require (a) analytical knowledge regarding metal flow, stresses and heat transfer as well as (b) technological information related to lubrication, heating...