1-20 of 103 Search Results for

arc spraying

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... Abstract This chapter discusses coating technologies that are applicable to beryllium, including physical and chemical vapor deposition, thermal evaporation, electroplating, sputtering, ion plating, and plasma arc spraying. It describes the advantages and disadvantages of each method and the...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290023
EISBN: 978-1-62708-306-5
.... With its low ionization potential, argon promotes easy arc starting and stable arc operation. Its lower thermal conductivity promotes the development of axial “spray” transfer in certain forms of GMAW. It is also used in applications where base material distortion must be controlled or where good gap...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... Abstract Casting is the most economical processing route for producing titanium parts, and unlike most metals, the properties of cast titanium are on par with those of wrought. This chapter covers titanium melting and casting practices -- including vacuum arc remelting, consumable electrode arc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
... Abstract This chapter discusses the processes, procedures, and equipment used in the production of iron, steel, aluminum, and titanium alloys. It describes the design and operation of melting and refining furnaces, including blast furnaces, basic oxygen and electric arc furnaces, vacuum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... conditioning systems, aluminum heat exchangers are essential components. Conventionally, these aluminum heat exchangers have been produced via a complex fabrication process that includes wire arc spraying, dipping, and brazing. In this process, zinc is sprayed onto aluminum brazing tubes to improve corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460017
EISBN: 978-1-62708-285-3
... shows typical microstructures of copper coatings as prepared by arc spraying and cold spraying. For the arc-sprayed coating, there is an oxygen content of 1.5 wt%, resulting in 30% lower electrical conductivity as compared to the initial high-conductivity oxygen-free copper powder ( Ref 2.28 ). In...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780153
EISBN: 978-1-62708-281-5
... natural sunlight, will influence test results on plastics. The use of a xenon arc weathering device is cited in ASTM G 26-84 ( Ref 4 ). There are four test methods outlined: Method 1 is a continuous exposure to light with an intermittent water spray. Method 2 is an alternating exposure to...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
... describes several welding processes, including arc welding, resistance welding, and friction stir welding, and addresses related issues such as welding defects, quality control, and stress relieving. The chapter also covers mechanical fastening techniques along with adhesive bonding and brazing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240349
EISBN: 978-1-62708-251-8
... steel: the electric arc furnace and the basic oxygen furnace. It also provides information on the classification and specifications for various steels, namely, plain carbon steels, low-carbon steels, medium-carbon plain carbon steels, and high-carbon plain carbon steels. The chapter concludes with a...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... overlays, thermal spraying, and various deposition technologies. ceramic coating chemical vapor deposition cladding corrosion resistance electroless plating electroplating hot dip metallic coating physical vapor deposition thermal spraying weld overlays THE SURFACE-ENGINEERING METHODS...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... be manipulated for complete coverage of the substrate. Processes for thermal spray coatings can be classified into two categories, arc processes and gas combustion processes, depending on the means of achieving the heat for melting of the consumable material during the spraying operation. The...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280117
EISBN: 978-1-62708-267-9
..., ESR VIM, VAR, ESR VIM; ceramic crucible Melting 2 … … Argon arc Plasma … Melt disintegration system/environment Nozzle; argon stream Expansion of dissolved hydrogen against vacuum and Ar + H 2 mixture Rotating consumable electrode; argon or helium Rotating consumable electrode; argon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... structures are more difficult to produce due to the need to hot isostatically press the cast structure for optimum properties. It is claimed that cast Ti-48Al-2Cr-2Nb alloy can be welded by the gas-tungsten arc welding process and by electron beam welding. By casting large structures in segments, hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
..., castlike structure. The spray gun generates the necessary heat for melting through combustion of gases, electric arc, or a plasma. The deposited structures of thermal spray coatings differ from those of the same material in the rough form because of the incremental nature of the coating buildup and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
...: Ref 25 Aluminum arc-spray coatings exhibit excellent corrosion resistance in marine environments, but are not recommended for use on conventional graphite/aluminum MMCs. The reduced thickness of the surface foils on these composites (0.13 to 0.18 mm, or 5 to 7 mils) prohibits grit blast surface...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... characteristics of various weld overlay coatings Table 15 Compares the applications of thermal spraying, welding, and electroplating Table 16 Compares the process requirements in thermal spraying, welding, and electroplating Table 17 Compares the design characteristics of flame, arc wire, high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... discontinuous aluminum MMCs include various casting processes, liquid metal infiltration, spray deposition, and PM. Each of these processes is briefly reviewed in the following sections. Particle-reinforced TMCs are processed by PM methods. Although a variety of materials have been...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240395
EISBN: 978-1-62708-251-8
... particles. Some alloy compositions have tungsten carbide additions to further improve wear resistance. Hardfacing materials are applied by either welding or thermal spraying. Weld overlay is a form of hardfacing that is applied by oxyacetylene or an arc welding process using hardfacing welding rods or...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080259
EISBN: 978-1-62708-304-1
... cladding in the boiler on the affected waterwall area with a corrosion-resistant alloy using automatic gas-metal-arc welding (GMAW) process. Cladding of waterwall panels can also be applied in shop using either GMAW or laser cladding techniques, and the cladded panels are then installed in the boiler. The...