Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300013
EISBN: 978-1-62708-323-2
... . Each additive has a function, like improves viscosity, prevents foaming, contains detergent (keeps system clean), is an antiwear agent, is a corrosion inhibitor, etc. The petroleum industry is evolving from the use of mineral oils for base oils to synthetic oils, but it may take some more decades...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300391
EISBN: 978-1-62708-323-2
... for an application. Every tribosystem manufacturer should tell users what type of oil to use. However, some aspects of oil additives are currently in flux with particles and antiwear additives. As is the case with oils, there are many tribotests to assess the life and lubricity of greases. Users must decide...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... described in this chapter are those that involve an intentional buildup or addition of a new layer on a metal substrate, that is, the application of a coating or lining. A wide range of processes are used to deposit metal, ceramic, and organic (paints or plastic and rubber linings) coatings or combinations...