Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980417
EISBN: 978-1-62708-342-3
... extrusion, the tool set for the production of section, rod, and round and shaped tubes is located in a tool holder. This is a cassette in Fig. 7.1 . Previously, tool heads, tool slides, or rotating arms were used. Fig. 7.1 Assembly of the tool set in a direct tube extrusion press. Source: Ames...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320185
EISBN: 978-1-62708-347-8
.... The cleaner the material is (AMS 2300), the higher the cost will be. Sometimes, selection of high-cost materials (vacuum-melted, high-alloy clean steel) helps to achieve an optimum gear design. It is thus important to develop a table of standard materials on the basis of overall cost. Table 10.1 shows...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090341
EISBN: 978-1-62708-266-2
.... Am. Ceram. Soc. , Vol 50 , 1967 , p 407 – 415 10.1111/j.1151-2916.1967.tb15145.x 14.2 Freiman S.W. , Effects of Chemical Environments on Slow Crack Growth in Glasses and Ceramics , J. Geophysical Res. , Vol 89 , 1984 , p 4072 – 4076 10.1029/JB089iB06p04072 14.3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... ( Ref 8.9 – 8.12 ). In particular, the application of the cold spray process to the automotive industry is being increasingly investigated. Such cold spray application research for the automotive industry can be broadly divided into three parts: additive manufacturing (AM) of components, fabrication...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120013
EISBN: 978-1-62708-269-3
... or strip (prEN2128) and forgings (prEN2522 and 2525) 0.05 0.08 0.012 0.2 0.2 0.4 total others … … … … 2.0–3.0Cu Ti-5Al-2.5Sn (UNS designation R54520) DIN17851 (alloy WL3.7115) 0.05 0.08 0.02 0.5 0.2 … 4.0–6.0 2.0–3.0 … … … AMS 4910 (plate, sheet, strip) 0.05 0.08 0.02...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... of Cemented Carbide , Powder Metall. , Vol 30 , 1987 , p 175 – 181 10.1179/pom.1987.30.3.175 19. Bae S.I. and Baik S. , Critical Concentration of MgO for the Prevention of Abnormal Grain Growth in Alumina , J. Am. Ceram. Soc. , Vol 77 , 1994 , p 2499 – 2504 10.1111/j.1151-2916.1994...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250059
EISBN: 978-1-62708-287-7
... Company of Brooklyn, 1865 2. Haynes E. , Materials for Automobiles , ASME Trans. , Vol 29 ( No. 1148 ), 1907 , p 209 – 16 3. Chapin W.R. , Properties of Some Steels in the Hardening Range , Trans. Am. Soc. Steel Treating , Vol 2 , 1922 , p 507 – 15 4. Davenport...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780089
EISBN: 978-1-62708-281-5
... Programs via Size Exclusion Chromatography . The WStatistic Concept, Am. Lab. , Jan 1985 , p 86 – 90 14. McCrary T.J. Jr. , Quality Assurance Programs via Size Exclusion Chromatography: Part Two, WStatistic Regression Equations for Physical Property Correlations , Am. Lab. , Feb...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250155
EISBN: 978-1-62708-345-4
... manufacturing and material procurement: Grade of steel with Aerospace Material Specification (AMS), if applicable AMS specification for material cleanliness, if required Hardnesses on tooth surface and at the core AGMA gear quality level Each hardness callout should have at least a range...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320021
EISBN: 978-1-62708-347-8
... ... ... ... ... 34 38.5 71.5 ... ... (a) Load, 3000 kgf; diam, 10 mm (0.4 in.) Distortion ratings of through-hardened gears Table 4.3 Distortion ratings of through-hardened gears Material AMS specification AMS quality Hardness (HRC) Distortion rating AISI 4340 6414 2300 48/50...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320033
EISBN: 978-1-62708-347-8
... Distortion ratings of common gear materials Material AMS specification AMS quality Quench media Hardness, HRC Distortion rating (a) Case Core AISI 8620 6276, 6277 2304 Oil 58–60 28–32 Fair AISI 9310/9315 6265 (b) , 6414 (c) 2300/2304 Oil 58–62 34–42 Fair AISI 4320 6299...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850334
EISBN: 978-1-62708-260-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... 209 – 219 10.1016/0956-7151(91)90269-7 3. Adcock D.S. and McDowall I.C. , The Mechanism of Filter Pressing and Slip Casting , J. Am. Ceram. Soc. , Vol 40 , 1957 , p 355 – 360 10.1111/j.1151-2916.1957.tb12552.x Selected References Selected References • Abolhasani...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
...-hardenable alloys Table 4 Compositions of semiaustenitic precipitation-hardenable alloys Alloy Designation C Mn Si Cr Ni Mo Al N 17-7 PH S17700 0.1 0.5 0.3 17 7.1 … 1 0 15-7 PH S15700 0.1 0.5 0.3 15 7.1 2.2 1 0 AM-350 S35000 0.1 0.8 0.4 17 4.3 2.8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
.... Mater. , Vol 122–123 ( No. 1–3 ), p 1417 – 1424 10.1016/0022-3115(84)90278-2 Bolomey R.A. , and Wish L.J. , 1950 . Thenol Trifluoride Acetone as a Complexing Agent for Isolation and Purification of Carrier-Free Radioberyllium , J. Am. Chem. Soc. , Vol 72 , p 4483 – 4486 10.1021...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.htpa.t53310119
EISBN: 978-1-62708-346-1
... claws Shore A0 according to ISO 7619-1 or Shore E according to ASTM D 2240 Rubbers in the range of low hardness, including foam rubber Shore AM according to ISO 7619 or Shore M according to ASTM D 2240 Thin rubber samples in the normal hardness range Shore B according to ASTM D 2240 Medium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060163
EISBN: 978-1-62708-355-3
... , 1978 , p 1 – 29 . 4. Lewis D. , Curve-Fitting Techniques and Ceramics , Am. Ceram. Soc. Bull. , Vol 57 (No. 4 ), 1978 , p 434 – 437 . 5. Weibull W. , A Statistical Distribution Function of Wide Applicability , J. Appl. Mech. , Vol 18 , 1951 , p 293 – 297 . 10.1115...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290067
EISBN: 978-1-62708-319-5
... and Compacting Performance of Spray Dried Molybdenum Powders , Int. J. Refract. Met. Hard Mater. , Vol 20 , 2002 , p 175 – 180 10.1016/S0263-4368(01)00062-2 3. Dhara S. and Bhargave P. , Egg White as an Environmentally Friendly Low-Cost Binder for Gelcasting Ceramics , J. Am. Ceram. Soc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.9781627082693