1-20 of 510 Search Results for

aluminum plating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630211
EISBN: 978-1-62708-270-9
... of the aluminum will be much more rapid in the same environment. Use a large anode metal and a small cathode metal to take advantage of the area effect. For example, plain steel rivets through aluminum sheet or plate may be satisfactory, but aluminum rivets through steel will corrode rapidly in an electrolyte...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... dimensions in an aluminum plate would not be considered corrosion failure. On the other hand, an aluminum roofing sheet may experience some shallow pitting and staining to the extent that its appearance changes. This can be considered either an aesthetic corrosion failure or acceptable corrosion resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
... at slow speeds, a necessary requirement for the high-strength alloys to prevent cracking. Typical casting speeds are in the range of 2.5 to 13 cm/min (1 to 5 in./min). Rolling Aluminum Plate and Sheet Titanium for ingot production may be either titanium sponge or reclaimed scrap (revert). In both...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... Aluminum Alloy Designation 2.4 Aluminum Alloys 2.5 Wrought Non-Heat-Treatable Alloys 2.6 Wrought Heat Treatable Alloys 2.7 Melting and Primary Fabrication 2.8 Rolling Plate and Sheet 2.9 Extrusion 2.10 Forging 2.11 Heat Treating 2.12 Annealing 2.13 Forming 2.14 Casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540169
EISBN: 978-1-62708-309-6
... 4.57. Liu A.F. , Crack Growth and Failure of Aluminum Plate under In-Plane Shear , AIAA J. , Vol 12 , 1974 , p 180 – 185 10.2514/3.49189 4.58. Shah R.C. , Fracture Under Combined Modes in 4340 Steel , Fracture Analysis , STP 560, ASTM, 1974 , p 29 – 52 4.59...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850001
EISBN: 978-1-62708-260-0
... Figure 1-1 Cold etch of disc cut from small ingot (10% aqueous HNO 3 ). Figure 1-2 Macrostructure of centrifugally cast 99.8% aluminum after a minor amount of reduction (3¼ ×; etchant, solution of 5 mL HNO 3 , 5 mL HCl, 5 mL HF, and 95 mL H 2 O). (Courtesy of R. D. Buchheit...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... the 2 xx , 3 xx , and 7 xx series. Mechanical Properties Physical Properties Wrought aluminum products can be divided into two groups. Standardized wrought products include sheet, plate, foil, rod, bar, wire, tube, pipe, and structural forms. Engineered wrought products are those designed...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870219
EISBN: 978-1-62708-299-0
.... , “ Exfoliation Test Results on 2519-T87 Plate: Disparity of Results in EXCO versus Other Environments ,” presentation of ASTM Subcommittee GO 1.05 Workshop on Exfoliation Corrosion ( Baltimore, MD ), 17 May 1988 16. Thompson J.J. , Exfoliation Corrosion Testing of Aluminum-Lithium Alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... iron Aluminum alloys 5052, 3004, 3003,1100, 6053 (in this order) Cadmium Aluminum alloys 2117, 2017, 2024 (in this order) Low-carbon steel Wrought iron Cast iron Ni-Resist (high-nickel cast iron) Type 410 stainless steel (active) 50-50 lead-tin solder Type 304 stainless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... of the space shuttle orbiter and cold plates in electronic microchip carrier multilayer boards. Fabrication processes for boron/aluminum composites are based on hot-press diffusion bonding of alternating layers of aluminum foil and boron fiber mats (foil-fiber-foil processing) or plasma-spraying methods...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
...) Nickel-base alloys (passive) Cu-35%Zn brass Nickel-base alloys (active) Manganese bronze Cu-40%Zn Tin Lead 316 stainless steel (active) 50%Pb-50%Sn solder 410 stainless steel (active) Cast iron Low-carbon steel 2024 aluminum 2017 aluminum Cadmium Alclad...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... on steel Low Antimony plate on steel Low Tin on steel Low Aluminum on aluminum Low Zinc-plated steel on aluminum Low Iron-plated steel on aluminum Low Cadmium on steel Medium Zinc on steel Medium Copper alloys on steel Medium Zinc on aluminum Medium Copper plate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
... design alternative is to TIG-weld a 6061 alloy aluminum plate on the underside of the central non-cored channel section, to improve the stiffness. The intermediate cross members that support the transmission and the rear cross members for the chassis are medium-to small-sized and do not pose...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... effect. Alloy 7072, Al-lZn, has a more anodic potential than pure aluminum and is used as the cladding for Alclad 3003, 5052, 6061, and 7075, as well as others. The most widely used alclad products are sheet and plate, although wire, tube, and other forms are also produced. The most generally...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540397
EISBN: 978-1-62708-309-6
... Alloy Plate—Tension Test of Large Center Slotted Panels , J. Mater. , Vol 2 , 1967 , p 889 – 914 A7.7. Staley J.T. , Microstructure and Toughness of Higher Strength Aluminum Alloys , STP 605, ASTM , 1976 A7.8. Bucci R.J. , Nordmark G. , and Starke E.A., Jr...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260087
EISBN: 978-1-62708-336-2
... plate die without backer and die ring Fig. 11 Comparison of feeder and recess dies Fig. 12 Recessed die. Source: Cardinal Aluminum Co. Fig. 13 Feeder plate die. (a) Complete die set with backer sitting behind die. (b) Die and backer Fig. 15 Porthole die. Source...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870101
EISBN: 978-1-62708-314-0
... aluminum project plate tool was identified as Tool “B.” Although it is used to make the same aircraft part as Tool “A,” the design concept is entirely different. Tool “B” consists of a thick aluminum slab 2.2 to 2.3 in. (56 to 58 mm) that was NC machined to the moldline contour on one surface and flat...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Plating Electroless Copper Plating Hot dip coating processes are used to apply coatings of zinc, zinc-iron, aluminum, aluminum-silicon alloy, Zn-5Al alloy, 55Al-Zn alloy, and lead-tin alloy to carbon steels. Metals such as chromium and titanium cannot be applied to steel by hot dipping because...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140175
EISBN: 978-1-62708-335-5
..., die cast. Specimen: 3 16 in. thick plate Fig. D2.31 Growth curves for aluminum alloy 380.0-F, die cast. Specimen: 3 16 in. thick plate Fig. D2.32 Growth curves for aluminum alloy 384.0-F, die cast. Specimen: 5 16 in. thick plate Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
... Dorward R.C. and Hasse K.R. , “ Flaw Growth of 7075, 7475, 7050, and 7049 Aluminum Plate in Stress Corrosion Environments ,” Final Technical Report for U.S. Government Contract NAS 830890, Oct 1976 ; Corrosion , Vol 34 ( No. 11 ), 1978 , p 386 – 395 10.5006/0010-9312-34.11.386 17.41...