1-20 of 347 Search Results for

aluminum die casting alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
... Abstract This chapter is a collection of tables listing: cast alloy designations of Aluminum Association, along with their general applications; the chemical compositions of the frequently used alloys for gravity permanent molds, low-pressure permanent molds, squeeze castings, and die castings...
Image
Published: 01 December 2004
Fig. D1.40 Room-temperature aging characteristics for aluminum alloy 413.0-F, die cast More
Image
Published: 01 December 2004
Fig. D1.41 Room-temperature aging characteristics for aluminum alloy 443.0-F, die cast More
Image
Published: 01 December 2004
Fig. D1.106 High-temperature aging characteristics for aluminum alloy 380.0-F, die cast More
Image
Published: 01 December 2004
Fig. D2.30 Growth curves for aluminum alloy 360.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.31 Growth curves for aluminum alloy 380.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.32 Growth curves for aluminum alloy 384.0-F, die cast. Specimen: 5 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.33 Growth curves for aluminum alloy 413.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.35 Growth curves for aluminum alloy 443.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.40 Growth curves for aluminum alloy 518.0-F, die cast. Specimen: 3 16 in. thick plate More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170432
EISBN: 978-1-62708-297-6
... is subsequently charged into the melting furnace with a proportion of process scrap. In some die-casting operations, the amount of process scrap generated is low, and it becomes economically feasible to have this scrap remelted and ingotted before it is reused. With the magnesium-aluminum-zinc alloys used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... technologies used with castings, including metallurgical bonding, metal-matrix composites, and hot isostatic pressing. aluminum alloy castings expendable mold gravity-feed casting nonexpendable mold gravity feed casting pressure die casting 3.1 History Aluminum alloy castings were first...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340083
EISBN: 978-1-62708-427-7
... of Leitelt Brothers Inc. and (b) a precision high-vacuum die casting of integral motorcycle frame. Courtesy of Suzuki DURING THE EARLY PHASE of the aluminum industry in the 1890s, castings made up the first type of manufactured product from aluminum (except in cases of aluminum as alloying with other...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170520
EISBN: 978-1-62708-297-6
...-drawn hardware, address plates, electrical components Zn-Al (superplastic zinc) Shaped components such as typewriter casings, computer panels, and covers Zinc Casting Alloys Zinc casting alloys can be divided into two principal classes based on aluminum content: the hypoeutectic die...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140175
EISBN: 978-1-62708-335-5
... Fig. D2.29 Growth and hardness curves for aluminum alloy 356.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 980 °F, boiling water quench. Comparison of sand cast and permanent mold Fig. D2.30 Growth curves for aluminum alloy 360.0-F, die cast. Specimen: 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140299
EISBN: 978-1-62708-335-5
... Abstract This appendix contains abbreviations and symbols related to aluminum alloy castings. aluminum alloy castings aluminum alloys symbols Aluminum Alloy Castings: Properties, Processes, and Applications Copyright © 2004 ASM International® J. Gilbert Kaufman and Elwin L. Rooy All...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140133
EISBN: 978-1-62708-335-5
...-temperature aging characteristics for aluminum alloy 356.0-T6. Effect of time interval between quenching and aging Fig. D1.38 Room-temperature aging characteristics for aluminum alloy 364.0-T4, die cast Fig. D1.39 Room-temperature aging characteristics for aluminum alloy 380.0-T5, die cast...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
... that covers production, quality assurance, properties, and applications of aluminum alloy castings. Unlike most sources, the content addresses not only conventional sand and permanent mold castings, but also pressure die castings and many of the variations of all three that have developed over the years...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340165
EISBN: 978-1-62708-427-7
..., process steps, alloys, and products of aluminum forging. aluminum alloys fatigue resistance forging fracture resistance Hot die forging of aluminum wheels at Weber Metals FORGING is the most basic, but perhaps most diverse, of the wrought metal processes. Most forging is carried out...