Published: 01 December 2004
Fig. D2.1 Growth curves for aluminum alloy 238.0-F, permanent mold. Test specimen: 1.125 diam × 12 in. rod More
Image
Published: 01 December 2004
Fig. D2.5 Growth curves for aluminum alloy 295.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.6 Growth curves for aluminum alloy B295.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 950 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.7 Hardness curves for aluminum alloy B295.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 940 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.9 Growth curves for aluminum alloy 319.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.10 Hardness curves for aluminum alloy 319.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.14 Growth curves for aluminum alloy 336.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 950 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.15 Hardness curves for aluminum alloy 336.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 950 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.16 Growth curves for aluminum alloy 355.0-F, permanent mold. Specimen: 1.125 diam × 12 in. rod More
Image
Published: 01 December 2004
Fig. D2.17 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 940 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.18 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.20 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 1000 °F, boiling water quench More
Image
Published: 01 December 2004
Fig. D2.21 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 940 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.22 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 960 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.23 Growth curves for aluminum alloy 355.0-T4, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 12 h at 1000 °F, cold water quench More
Image
Published: 01 December 2004
Fig. D2.24 Growth curves for aluminum alloy 355.0-T51, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 8 h at 440 °F More
Image
Published: 01 December 2004
Fig. D2.25 Growth curves for aluminum alloy 355.0-T7, permanent mold. Specimen: 1.125 diam × 12 in. rod. Treatment: 5 h at 700 °F plus 12 h at 850 °F, boiling water quench, 8 h at 440 °F More
Image
Published: 01 December 2004
Fig. D2.30 Growth curves for aluminum alloy 360.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.31 Growth curves for aluminum alloy 380.0-F, die cast. Specimen: 3 16 in. thick plate More
Image
Published: 01 December 2004
Fig. D2.32 Growth curves for aluminum alloy 384.0-F, die cast. Specimen: 5 16 in. thick plate More