1-3 of 3 Search Results for

aluminum alloy 7150-T7751 plate

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340179
EISBN: 978-1-62708-427-7
... plate with poor exfoliation performance compared with the specially developed T7751 temper. Fig. 9.22 Exfoliation corrosion attack in 7150-T76151 plate Fig. 9.23 Alloy 7150 plate samples after exposure to coastal atmosphere, (a) T7751 and (b) T6151 Stress Corrosion Cracking...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240487
EISBN: 978-1-62708-251-8
... 51 290 42 13 7049 T73 Forging 540 78 475 69 10 7050 T74, T745X Plate, forging, extrusion 520 74 450 65 13 7150 T651, T6151 Plate 600 87 560 81 11 T77511 Extrusion 650 94 615 89 12 7055 T7751 Plate 640 93 615 89 10 T77511 Extrusion 670 97 655...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... 51 290 42 13 7049 T73 Forging 538 78 476 69 10 7050 T74, T745X Plate, forging, extrusion 510 74 448 65 13 7150 T651, T6151 Plate 600 87 559 81 11 T77511 Extrusion 648 94 614 89 12 7055 T7751 Plate 641 93 614 89 10 T77511 Extrusion 669 97 655...