1-9 of 9 Search Results for

aluminum alloy 7020

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080423
EISBN: 978-1-62708-304-1
...Results of static immersion tests in molten aluminum at 760 °C (1400 °F) for 4 h Table 16.1 Results of static immersion tests in molten aluminum at 760 °C (1400 °F) for 4 h Alloy Maximum depth of corrosion attack, mm (mils) Titanium 0.22 (8.5) 6B 0.43 (16.8) 188 0.51 (20.2...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410133
EISBN: 978-1-62708-265-5
.... , Solubility of Gaseous Nitrogen in Gamma Iron and the Effect of Alloying Constituents—Aluminum Nitride Precipitation , Trans. AIME , Vol 191 , 1951 , p 1174 – 1179 10.1007/BF03397430 8.31 Melloy G.F. , Austenite Grain Size—Its Control and Effects , Metals Engineering Institute, American...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260149
EISBN: 978-1-62708-336-2
...Abstract Abstract This chapter discusses the extrusion characteristics of relatively soft aluminum alloys. It begins by identifying alloy designations within the class and the types of extrusions made from them. It then explains how extruded shapes and cross-sections are defined and how...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980567
EISBN: 978-1-62708-342-3
...Abstract Abstract This appendix contains tables listing the approximate composition of materials for the extrusion process. The materials covered are aluminum alloys, magnesium and magnesium alloys, copper and copper alloys, cobalt alloys, nickel and nickel alloys, iron alloys, steels, lead...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980417
EISBN: 978-1-62708-342-3
... of the extrudability of specific aluminum alloys Table 7.2 Bearing length addition as a function of the extrudability of specific aluminum alloys Extrudability Alloys Easy Moderate Difficult Addition, % None 15 30 Material 1350 5049 2014A 6060 5051A 2017A 6082 5251 2024 7020...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080097
EISBN: 978-1-62708-304-1
... of pressure. Source: Ref 95 Fig. 5.68 Metal dusting resistance of Fe-Ni-Cr alloys (800H and HP40) in comparison with Ni-base alloy 600H tested at 650 °C (1200 °F) in H 2 -24CO-2H 2 O ( a c = 14). Source: Ref 94 Fig. 5.69 Increasing Cr along with addition of aluminum improves...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... enable a wide spectrum of materials to be extruded. This chapter focuses on the processes involved in the extrusion of semifinished products in various metals and their alloys, namely tin, lead, lead-base soft solders, tin-base soft solders, zinc, magnesium, aluminum, copper, titanium, zirconium, iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220193
EISBN: 978-1-62708-259-4
...Abstract Abstract Heat treatment is the most common way of altering the mechanical, physical, and even chemical properties of steels. This chapter describes the changes that occur in carbon and low-alloy steels during conventional heat treatments. It explains how austenite decomposition largely...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1