1-12 of 12 Search Results for

aluminum alloy 6201

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340413
EISBN: 978-1-62708-427-7
... strands of a stronger aluminum alloy, typically 6201-T8 with an EC of approximately 54% IACS. This product is referred to as aluminum conductor, alloy reinforced (ACAR) . Figure 18.1 shows examples of some of the many ACAR stranding arrangements. The strengths of the composite (ACSR or ACAR) cables...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870161
EISBN: 978-1-62708-299-0
... susceptible to stress-corrosion cracking (SCC). More detailed information on the joining methods discussed in this chapter can be found in Welding, Brazing, and Soldering , Volume 6, of the ASM Handbook; the ASM Specialty Handbook: Aluminum and Aluminum Alloys; and Adhesives and Sealants , Volume 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820143
EISBN: 978-1-62708-339-3
... aluminum filler alloys used to fillet weld or butt weld two component base alloys, where one of the base alloys is 6005, 6063, 6101, 6151, 6201, 6351, or 6951 Table 3(e) Relative rating of selected aluminum filler alloys used to fillet weld or butt weld two component base alloys, where one of the base...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930283
EISBN: 978-1-62708-359-1
... Abstract This article reviews weldability of aluminum alloys and factors that affect weld performance. It first addresses hot tears, which can form during the welding of various aluminum alloys. It then presents comparison data from different weldability tests and discusses the specific...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090241
EISBN: 978-1-62708-266-2
... Abstract Aluminum is protected by a barrier oxide film that, if damaged, reforms immediately in most environments. Despite this inherent corrosion resistance, there are conditions where aluminum alloys, like many materials, are subject to the effects of stress-corrosion cracking (SCC...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870025
EISBN: 978-1-62708-299-0
... Abstract Aluminum generally has excellent resistance to corrosion and gives years of maintenance-free service in natural atmospheres, fresh waters, seawater, many soils and chemicals, and most foods. This chapter explains why aluminum and aluminum alloys are naturally resistant to corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170351
EISBN: 978-1-62708-297-6
... Abstract This article discusses the composition, structures, properties, and behaviors of aluminum alloys and explains how they correspond to specific alloying elements. It begins with an overview of the general characteristics of wrought and cast aluminum alloys, the four-digit classification...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... Abstract Aluminum is the second most widely used metal in the world. It is readily available, offers a wide range of properties, and can be shaped, coated, and joined using a variety of methods. This chapter discusses some of the key attributes of wrought and cast aluminum alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870251
EISBN: 978-1-62708-299-0
... Abstract This appendix contains composition limit data for wrought aluminum and aluminum alloys. aluminum alloys chemical composition wrought aluminum alloys Composition limits for wrought aluminum and aluminum alloys Table A-1 (Part 1) Composition limits for wrought aluminum...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... Abstract This chapter provides basic engineering information on aluminum alloys with an emphasis on their use in applications where weight is a significant design factor. It discusses the advantages and limitations of various types of aluminum along with their compositions, designations...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... Aluminum 0–6 0–4.5 Titanium 0–6 0–4 Cobalt 0–20 … Nickel … 0–22 Niobium 0–5 0–4 Tantalum 0–12 0–9 Rhenium 0–6 0–2 Role of alloying elements in superalloys Table 1(b) Role of alloying elements in superalloys Effect (a) Iron-base Cobalt-base Nickel-base...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6