DOI: 10.31399/asm.tb.ffub.t53610209
EISBN: 978-1-62708-303-4
... of purity on toughness of other alloys is shown in Table 4 . Fig. 27 Aluminum alloys 2124 and 7475 are tougher versions of alloys 2024 and 7075. High-purity metal (low iron and silicon) and special processing techniques are needed to optimize toughness in these materials. Source: Ref 13...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540397
EISBN: 978-1-62708-309-6
... is higher in the high-purity alloys (designated as 2124 and 7475). Source: Ref A7.2 Fig. A7.2 Plane-strain fracture toughness as a function of material tensile yield strength. Comparison of several 2000 and 7000 series aluminum alloys. Source: Ref A7.1 Fig. A7.3 Plane-strain fracture...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870063
EISBN: 978-1-62708-299-0
... corrosion. In the heat treatable aluminum-copper-magnesium (2 xxx ) and aluminum-zinc-magnesium-copper (7 xxx ) alloys, exfoliation corrosion has usually been confined to relatively thin sections of highly worked products with an elongated grain structure. In 2124-T351 plate, for example, 13 mm (0.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870045
EISBN: 978-1-62708-299-0
... example demonstrates the use of coatings to minimize crevice corrosion aboard the space shuttle. The exterior window frames on the space shuttle orbiter are made of aluminum alloy 2124-T851 that has been anodized according to a Rockwell specification by using a sulfuric acid anodize, a black dye...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
... that has since been adopted by the American National Standards Institute (ANSI) in ANSI 35.5-1992, using the following format: matrix/reinforcement/vol% form. For example, 2124/SiC/25w describes alloy 2124 reinforced with 25 vol% of silicon carbide whiskers; 7075/Al 2 O 3 /10p is the alloy 7075...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870099
EISBN: 978-1-62708-299-0
.... Stress-Corrosion Cracking Corrosion Fatigue Liquid-Metal Embrittlement References References 1. Summerson T.J. and Sprowls D.O. , Corrosion Behavior of Aluminum Alloys , International Conference of the Hall-Heroult Process Vol III of Conf. Proc. , ( University of Virginia...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040211
EISBN: 978-1-62708-300-3
... ductility at room temperature can be cold forged. This group consists primarily of steels and aluminum alloys. However, alloys of copper, zinc, tin, titanium, beryllium, and nickel are also cold forged for special applications [ Gentzsch, 1967 ]. Examples of steels that are used extensively...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... by Molten Aluminum Alloy , J. Mater. Process. Technol. , Vol 119 , 2001 , p 324 – 328 10.1016/S0924-0136(01)00975-X • Kaczmar J.W. , Pietrzak K. , and Wlosinski W. , The Production and Application of Metal Matrix Composites , J. Mater. Process. Technol. , Vol 106 , 2000 , p...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
...Abstract Abstract Aluminum is the second most widely used metal in the world. It is readily available, offers a wide range of properties, and can be shaped, coated, and joined using a variety of methods. This chapter discusses some of the key attributes of wrought and cast aluminum alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260187
EISBN: 978-1-62708-336-2
... of extrusion ratio on strength. Source: Ref 16 Abstract Abstract This chapter discusses the extrusion characteristics of hard aluminum alloys, particularly those in the 5000 and 7000 series. It begins with a review of two studies, one showing how the extrudability of 7 xxx alloys varies...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
...Abstract Abstract This chapter provides basic engineering information on aluminum alloys with an emphasis on their use in applications where weight is a significant design factor. It discusses the advantages and limitations of various types of aluminum along with their compositions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240221
EISBN: 978-1-62708-251-8
... of microstructural variables on fracture toughness of steels, aluminum alloys, and titanium alloys. fracture ductile fracture brittle fracture Griffith theory plane-strain fracture toughness temperature steels aluminum alloys titanium alloys notched bar impact testing microstructure FRACTURE...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... designation system for MMCs that has since been adopted by the American National Standards Institute (ANSI). ANSI 35.5-1992 provides that aluminum MMCs be identified as follows: Matrix/reinforcement/vol% form For example, 2124/SiC/25w describes the AA-registered alloy 2124 reinforced with 25 vol...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870251
EISBN: 978-1-62708-299-0
...Abstract Abstract This appendix contains composition limit data for wrought aluminum and aluminum alloys. aluminum alloys chemical composition wrought aluminum alloys Composition limits for wrought aluminum and aluminum alloys Table A-1 (Part 1) Composition limits for wrought...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090241
EISBN: 978-1-62708-266-2
...Abstract Abstract Aluminum is protected by a barrier oxide film that, if damaged, reforms immediately in most environments. Despite this inherent corrosion resistance, there are conditions where aluminum alloys, like many materials, are subject to the effects of stress-corrosion cracking (SCC...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240487
EISBN: 978-1-62708-251-8
.... This chapter examines the metallurgy, composition, processing, and mechanical properties of aluminum and its alloys, both cast and wrought forms. It also covers heat treating and basic temper designations, including annealed, work hardened, solution heat treated, and solution heated treated and aged...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610101
EISBN: 978-1-62708-303-4
... is used for high-strength metals, such as high-strength steels, titanium, and aluminum alloys. EPFM is used when the crack tip is not sharp and there is some crack tip plasticity (blunting). EPFM is used in the design of materials, such as lower-strength, higher-toughness steels. There are numerous...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310351
EISBN: 978-1-62708-326-3
... temperatures for selected aluminum alloys Table 8 Recommended solution heat treating temperatures for selected aluminum alloys Alloy Form Set temperature Notes °C °F 2004 Sheet 529 985 … 2014,   2017,   2117 All 502 935 … 2024,   2124,   2224 All 493 920 … 2098 All...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170351
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the composition, structures, properties, and behaviors of aluminum alloys and explains how they correspond to specific alloying elements. It begins with an overview of the general characteristics of wrought and cast aluminum alloys, the four-digit...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... elements   Minor elements   Impurities Some environment-alloy combinations known to result in SCC Table 7 Some environment-alloy combinations known to result in SCC Environment Alloy system Aluminum alloys Carbon steels Copper alloys Nickel alloys Stainless steels Titanium...