... Abstract This chapter is a collection of tables listing: cast alloy designations of Aluminum Association, along with their general applications; the chemical compositions of the frequently used alloys for gravity permanent molds, low-pressure permanent molds, squeeze castings, and die castings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... Abstract Aluminum casting alloy compositions parallel those of wrought alloys in many respects. However, because work hardening plays no significant role in the development of casting properties, the use and purposes of some alloying elements differ in casting alloys versus wrought alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870259
EISBN: 978-1-62708-299-0
... Abstract This appendix includes composition limit data for aluminum castings and ingots. aluminum alloys cast aluminum alloys chemical composition ingots Table A-2 (Part 1) Composition limits for unalloyed and alloyed aluminum castings ( xxx .0) and ingots ( xxx .1 or xxx .2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... Abstract This chapter begins with information on the historical development of aluminum alloy castings. It then covers the basic factors involved in the selection of a casting process. This is followed by sections describing the various categories of casting processes and their variants...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040025
EISBN: 978-1-62708-300-3
... a significant amount of experimentally derived flow stress data, including K and n values for steel, copper, and aluminum alloys, C and m values (at various temperatures) for steel, aluminum, copper, titanium, and other alloys, and average flow stress for several alloys determined by compression testing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170351
EISBN: 978-1-62708-297-6
..., forgings Table 5 Designations and nominal compositions of common aluminum alloys used for casting AA number Product (a) Composition, % Cu Mg Mn Si Others 201.0 S 4.6 0.35 0.35 … 0.7 Ag, 0.25 Ti 206.0 S or P 4.6 0.25 0.35 0.10 (b) 0.22 Ti, 0.15 Fe (b) A206.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140069
EISBN: 978-1-62708-335-5
... Abstract This chapter reviews and provides data tables for the wide range of properties and performance characteristics that are possible with specific aluminum casting alloys and tempers. Properties and performance attributes addressed include casting and finishing characteristics; typical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.9781627083003