... or monofilament fibers. Fig. 20.1 Metal matrix composite reinforcements. Source: Ref 1 Discontinuous reinforcements consist mainly of silicon carbide (SiC) in whisker (w) form; particulate (p) types of SiC, alumina (Al 2 O 3 ), and titanium diboride (TiB 2 ); and short or chopped fibers (c) of Al...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... deformation (a) Total deformed layer (b) Type Grade Abrasive cutoff wheel Alumina A 60 DE wheel Proprietary oil-water emulsion 4 16 700 Hand hacksaw 18 t.p.i., roll-set blade Nil 100 55 750 Surface grinding Alumina 28A 46 KVBE wheel 0.001-in feed, machine surface grinding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.tm.9781627083577
EISBN: 978-1-62708-357-7
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300271
EISBN: 978-1-62708-323-2
.... 10.2 Ceramics Alumina The ceramics most often used in tribosystems are sometimes given a prefix, such as advanced , fine , engineering , and so on, to distinguish them from flooring tiles. However, no term is agreed upon by manufacturers, because each has their own prefix for the big four...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230207
EISBN: 978-1-62708-351-5
... Substrate Filler metal Process temperature Remelt temperature Ref °C °F °C °F Alumina Cu/Ni/Cu interlayers 1150 1920 1400 2550 Shalz et al. [1994] Alumina/kovar Ni/Ti/Ni interlayers 980 1800 984–1310 1805–2390 Zhang, Qiao, and Jin [2002] Cobalt alloys Ni-4B 1175 2145...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400087
EISBN: 978-1-62708-258-7
... to ensure that there is no rounding of the edges of the coating. If rounded, the mound should be reground, starting at 600 grit until flat. Polishing: The specimens will be polished using an aqueous 1 μm alumina (Al 2 O 3 ) solution on a napless cloth. First, use a stationary wheel or flat surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440189
EISBN: 978-1-62708-352-2
... of this chapter outlines some of the reported attempts to find replacements for these alloys. One positive benefit of the switch to lead-free solders is elimination of the need to source low-alpha-emission solder for electronics applications. Lead, being a heavy metal, contains a proportion of radioactive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.9781627082839
EISBN: 978-1-62708-283-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850001
EISBN: 978-1-62708-260-0
.... The chemically absorbed layer was studied after diamond and alumina polishing using AES (auger electron spectroscopy) and SIMS (secondary ion mass spectrometry) techniques, which showed that this layer consisted of oxygen-metal compounds plus sulfur or ammonium compounds, depending on whether polishing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
...) crystal structure referred to as alpha (α) phase. At 883 °C (1621 °F), this transforms to a body-centered cubic (bcc) structure known as beta (β) phase. The manipulation of these crystallographic variations through alloying additions and thermomechanical processing is the basis for the development...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390284
EISBN: 978-1-62708-459-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860269
EISBN: 978-1-62708-348-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.9781627083003
EISBN: 978-1-62708-300-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870375
EISBN: 978-1-62708-344-7