Image
Published: 01 July 1997
Fig. 10 Effect of alloy composition (high alloy versus low alloy concentrations of iron, silicon, manganese, and sulfur taken collectively) on the cracking tendency of postweld heat-treated René. 41. Source: Ref 15 More
Image
Published: 01 March 2002
Fig. 9.9 Effect of alloy composition on cracking tendency of Rene 41 nickel-base superalloy. Showing effects of high alloy vs. low alloy concentrations of iron, silicon, manganese, and sulfur in the alloy More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000005
EISBN: 978-1-62708-312-6
... Abstract This chapter provides information on the properties and behaviors of stainless steels and stainless steel powders. It begins with a review of alloy designation systems and grades by which stainless steels are defined. It then describes the composition, metallurgy, and engineering...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... Abstract This appendix provides tables listing alloy compositions and standard designations and common unit and hardness conversion factors. chemical composition corrosion-resistant castings hardness heat-resistant castings low alloy steel wrought carbon steel wrought stainless...
Image
Published: 01 August 2005
Fig. 2.4 Copper-zinc phase diagram. The range of alloy compositions used as brazes is indicated. These are characterized by having narrow melting ranges. More
Image
Published: 01 December 2000
Fig. 3.1 Some U.S. alloy compositions relative to a pseudobinary titanium phase diagram More
Image
Published: 01 November 2007
Fig. 15.3 Composition of a Fe-1.8% C alloy on the iron-carbon phase diagram More
Image
Published: 01 August 2018
Fig. 8.24 The solidification of an alloy with a hypo-eutectic composition X 0 begins with the formation of austenite in accordance with the schematic phase diagram. As austenite forms, the interdendritic liquid gets richer in carbon until the composition of the eutectic, X E , is reached More
Image
Published: 01 June 1983
Figure 5.14 The variation of resistivity with composition for the magnetic alloy Cu-Ni, ○, Δ, and solid curves — Iguchi and Udagawa (1975) ; □ — Legvold, Peterson, Burgardt, Hofer, Lundell, Vyrostek, and Gartner (1974) ; • — Krupkowski and de Haas (1928) . Agreement with Svensson’s (1936 More
Image
Published: 01 June 1983
Figure 5.15 The variation of resistivity with composition for the magnetic alloy Ag–Pd. ○ — Svensson (1932) , Δ — Murani (1974) . More
Image
Published: 01 June 1983
Figure 7.9 Critical resolved shear stress as a function of composition in Ag—Au alloy single crystals ( Sachs and Weerts, 1930 ). More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1996
DOI: 10.31399/asm.tb.phtpclas.t64560415
EISBN: 978-1-62708-353-9
... Abstract This appendix contains tables listing the chemical compositions of standard alloy steels. This appendix is a reprint of tables giving compositions of standard alloy steels and standard boron (alloy) steels. Reproduced from Metal Progress Databook , American Society for Metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870251
EISBN: 978-1-62708-299-0
... Abstract This appendix contains composition limit data for wrought aluminum and aluminum alloys. aluminum alloys chemical composition wrought aluminum alloys Composition limits for wrought aluminum and aluminum alloys Table A-1 (Part 1) Composition limits for wrought aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... Abstract This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion-strengthened...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870259
EISBN: 978-1-62708-299-0
... Abstract This appendix includes composition limit data for aluminum castings and ingots. aluminum alloys cast aluminum alloys chemical composition ingots Composition limits for unalloyed and alloyed aluminum castings (<italic>xxx</italic>.0) and ingots (<italic>xxx</italic>.1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1996
DOI: 10.31399/asm.tb.phtpclas.t64560416
EISBN: 978-1-62708-353-9
... Abstract This appendix lists the chemical compositions of standard alloy H-steels and standard boron (alloy) H-steels. This appendix is a reprint of tables giving compositions of standard alloy H-steels and standard boron (alloy) H-steels. Reproduced from Metal Progress Databook...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170337
EISBN: 978-1-62708-297-6
... Abstract This article discusses the effect of alloying on the composition, structure, properties, and processing characteristics of ordered intermetallic compounds, including nickel aluminides, iron aluminides, and titanium aluminides. It includes several data tables along with a list...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... Abstract Aluminum casting alloy compositions parallel those of wrought alloys in many respects. However, because work hardening plays no significant role in the development of casting properties, the use and purposes of some alloying elements differ in casting alloys versus wrought alloys...
Image
Published: 01 August 2005
Fig. 2.32 An alloy microstructure characteristic of a (ternary) eutectic transformation. The alloy composition is 35.8Ag-34.2Al-30.0Ge. 100× More
Image
Published: 01 December 1995
Fig. 22-7 Comparison of standard HP grade, niobium-modified alloys, and micro-alloyed compositions—100,000 hour rupture lives More