1-20 of 283 Search Results for

abrasive

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630169
EISBN: 978-1-62708-270-9
...Abstract Abstract This chapter is a detailed account of the general characteristics and effects of and the methods for preventing or reducing different categories of wear failures, namely abrasive (erosive, grinding, and gouging), adhesive, and fretting wear. abrasive wear adhesive wear...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300079
EISBN: 978-1-62708-323-2
... 2000 Diamond (hardest) 10 10,000 Fig. 4.17 Scratch testing to simulate abrasion; scratch width is the test metric; w, width; P, scratch load Fig. 4.18 Schematic of (a) two-body and (b) three-body abrasion Fig. 4.19 Adhesive transfer to abrasive particles Fig...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
... test wear counterface, at a magnification of 15× Fig. 5.16 Abrasion wear scars at a magnification of 15×. (a) Two-body abrasion from 30 μm alumina in ASTM G174 abrasion test. (b) Three-body abrasion from 60 mesh silica in ASTM G65 abrasion test Fig. 5.19 A simple solid particle...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
... in continuous sliding versus a 440C stainless steel shaft at 58 HRC Fig. 6.5 Abrasion wear volume of some copper alloys compared with other metals using the ASTM G174 two-body abrasion test (procedure c, 200 g force, 1 km abrasion, 30 μm alumina abrasive) Fig. 6.6 Resistance of some copper...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... iron/chromium hardfacings Consumable Composition, % C Mn Cr Mo Si Fe RFeCr-A1 3.7–5 2–6 27–35 … 1.1–2.6 Rem EfeCo-A1 3–5 4–8 26–32 2 1–2.5 Rem Fig. 7.11 Abrasion of various metals using the ASTM G174 two-body abrasion test (200 g, 680 belt passes, 30 μm...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300199
EISBN: 978-1-62708-323-2
... pearlite (black) in the ferrite (white); (c) 1080 steel: the microstructure is almost entirely pearlite; (d) hardened 1080 steel: the microstructure is 100% martensite. Fig. 8.6 Railroad track spalling from rolling wear and surface fatigue Fig. 8.7 Three-body abrasion characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300301
EISBN: 978-1-62708-323-2
...) exists on the polystyrene molecule. n, number; H, hydrogen; C, carbon Fig. 11.5 Abrasion of an acrylonitrile butadiene styrene snow shovel Fig. 11.6 Three-body abrasion test results of various plastics using a reduced-cycle adaptation of ASTM International G65. UHMWPE, ultrahigh...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
...Abstract Abstract Metal-matrix composites (MMCs) work at higher temperatures than their base metal counterparts and can be engineered for improved strength, stiffness, thermal conductivity, abrasion and/or creep resistance, and dimensional stability. This chapter examines the properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780276
EISBN: 978-1-62708-281-5
..., goats, slideways bearings, and abrasive wear application PV < 15 MPa · m/s V < 5 m/s, μ > 0.03 T < 250 °C W S > 10 −16 m 3 /Nm Continuous-fiber-reinforced composites (UD) Underwater or high-temperature applications, netrospace scals and bearings PV < 100 MPa · m/s V...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
... of service temperatures. This chapter covers several types of component and material failure associated with wear, temperature effects, and crack growth. It examines temperature-induced, brittle, ductile, and fatigue failures as well as failures due to abrasive, erosive, adhesive, and fretting wear...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430314
EISBN: 978-1-62708-253-2
... of ferrite, bainite and carbides, 100× Abstract Abstract Combustion byproducts such as soot, ash, and abrasive particulates can inflict significant damage to boiler tubes through the cumulative effect of erosion. This chapter examines the types of erosion that occur on the fire side of boiler...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170107
EISBN: 978-1-62708-297-6
... matrix supporting the carbide phase can be adjusted via alloy content and heat treatment to optimize the balance between abrasion resistance and impact toughness. It also describes the effect of alloying elements and inoculants on various properties and behaviors and provides information on commercial...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
... machining processes such as electrical discharge, abrasive jet, and hydrodynamic machining, laser and electron beam machining, ultrasonic impact grinding, and electrical discharge wire cutting. chip formation cutting fluids cutting tools machinability machining tool wear MACHINING COVERS...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610461
EISBN: 978-1-62708-303-4
...Abstract Abstract This chapter discusses the causes and effects of wear along with prevention methods. It covers abrasive, erosive, erosion-corrosion, grinding, gouging, adhesive, and fretting wear. It also discusses various forms of contact-stress fatigue, including subsurface-origin fatigue...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120085
EISBN: 978-1-62708-269-3
... heated for 1 h at 425 °C(795 °F) Mass (barrel) finishing conditions for titanium parts Table 11.4 Mass (barrel) finishing conditions for titanium parts Capacity, Barrel size diam Width Speed, rev/min Part load Medium (a) Water Abrasive compound (b) Alkaline cleaner (c) m 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300271
EISBN: 978-1-62708-323-2
... Fig. 10.17 Cermet hardfacing containing carbide spheres in a metal matrix. Original magnification: 100× Fig. 10.18 Microstructure of titanium carbide cermet with a stainless steel matrix. Original magnification: 800× Fig. 10.19 Two-body abrasion test results of various...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780259
EISBN: 978-1-62708-281-5
...Kinetic coefficients of friction (dry and lubricated) and relative abrasion resistance for selected polymeric materials Table 3 Kinetic coefficients of friction (dry and lubricated) and relative abrasion resistance for selected polymeric materials Resin (a) Kinetic coefficient...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... Resistance , Prentice Hall , 1988 , p 15 – 43 3. Sedriks A.J. and Mulhearn T.O. , The Effect of Work-Hardening on the Mechanics of Cutting in Simulated Abrasive Processes , Wear , Vol 7 , 1964 , p 451 10.1016/0043-1648(64)90137-1 4. Sasaki T. and Okamura K...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
...Depth of plastically deformed layer produced on annealed polycrystalline 70:30 brass by machining, grinding, and abrasion processes Table 2-1 Depth of plastically deformed layer produced on annealed polycrystalline 70:30 brass by machining, grinding, and abrasion processes Process Depth...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2