1-20 of 484 Search Results for

Wire products

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480207
EISBN: 978-1-62708-318-8
.... extrusion forging rolling wrought titanium TITANIUM AND TITANIUM ALLOYS are fabricated using many methods to produce mill products, including billet, bar, rod, wire, plate, sheet, strip, extrusions, pipe, and tubing ( Ref 9.1 – 9.13 ). Most integrated titanium mills have primary working equipment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120295
EISBN: 978-1-62708-269-3
... Katternberger Strasse 155-159 Solingen 426455 Germany Dietmar Fischer    Tel: +49 (0) 201 188 2593    Fax: +49 (0) 201 188 3520 Stockist of titanium ingot, bar, plate, sheet, profile, tube, and wire products Rolls Laval P.O. Box 100 Wolverhampton WV4 6JY Steve Sproson    Tel: +44 (0) 1902 353353    Fax...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250219
EISBN: 978-1-62708-287-7
... for grinding mills at iron mines. In 1980, North Star built a minimill at Monroe, Michigan, to manufacture higher quality steel bars for the automotive industry. In 1983, the company purchased a mill at Beaumont, Texas, with a 500,000 ton capacity to make rod and wire products. They also bought a minimill from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410315
EISBN: 978-1-62708-265-5
... friction. High-Strength Patented and Cold-Drawn Pearlitic Steel Wire Pearlitic microstructures in steels of eutectoid composition are drawn to wires that have the highest useable tensile strengths of any steel products. The strengths depend on steel quality, the microstructure prior to wire drawing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780141
EISBN: 978-1-62708-268-6
... are not changed frequently. Sometimes, contaminants can be airborne. This may occur if dust or paints are present. Some processes use etchants with a subsequent rinse. Very small-diameter wires are produced by exposing a larger-diameter wire to an acid etch to reduce the diameter and then rinsing the wire...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
... from cars to appliances Wire, used in such products as bed springs, wire rope, nails, and wire fabric Structural shapes used in buildings and bridges Bars for forgings and machined parts, such as gears and bearings Steels powders are also produced for various applications, including...
Image
Published: 01 December 2000
Fig. 2.1 Some titanium and titanium alloys product forms. (a) Strip. (b) Slab. (c) Billet. (d) Wire. (e) Sponge. (f) Tube. (g) Plate. Courtesy of Teledyne Wah Chang Albany More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... as other industries and many consumer products. The thermal spray process requires a material in wire or powder form that is transferred to the surface by heat and/or kinetic energy, forming a protective layer. Thermal spray equipment basically consists of a spray gun, materials that are sprayed...
Image
Published: 01 December 2001
Fig. 21 Room-temperature hardness of two different low-alloy gray irons held at normalizing temperature 1 h for each 25 mm (1 in.) of thickness and air cooled on wire mesh screen. From production and experimental data More
Image
Published: 01 December 2006
Fig. 5.3 Modern integrated fully automatic 5000 kN extrusion plant for the production of bar, wire, tube, and sections in lead and tin alloys complete with casting oven, triple billet casting plant, hot-billet shear, and oil hydraulic long-stroke extrusion press (Source: Collin) More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720321
EISBN: 978-1-62708-305-8
... Handbook , ASM International , 1989 , p 549 – 560 2. Matsubara N. , Yamaguchi H. , Hiroshima T. , Sakamoto T. , and Matsumoto S. , Nondestructive Testing of Cold Drawn Wires and Cold Forged Products , Wire J. Int. , March 1986 ...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460173
EISBN: 978-1-62708-285-3
... spray powder production are the following: Crucible melting Crucible-free melting Wire-feed melting Crucible Melting Crucible melting of the feedstock can be performed by any of several heating techniques; again, the most common is induction heating. Once the material is fed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230295
EISBN: 978-1-62708-298-3
.... beryllium extrusion forging formability forming rolling spinning wire drawing THIS CHAPTER COVERS various metalworking methods used to manufacture a beryllium product, including rolling, forming, forging, extrusion, wire drawing, spinning, and near-net shape forming. The method normally used...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980001
EISBN: 978-1-62708-342-3
..., in which a billet, usually round, is pressed by a stem at high pressure through a tool of the desired shape, the die, to one or more lengths, first achieved its important position in the semifinished product industry in the twentieth century. The process was used mainly for the production of bar, wire...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... extruded. Fig. 6.16 Drawing process Drawing Drawing is one of the oldest metalforming operations to make long products with excellent surface finishes, closely controlled dimensions, and constant cross sections. Wire and tubes are drawn in a similar manner. The general practice is to place...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730149
EISBN: 978-1-62708-283-9
... of energy that is used to produce copper from ore. In general, the value of recycled copper is approximately 90% that of virgin copper. The primary sources are electrical wiring, plumbing pipes, and fixtures. Control of the scrap is important. To produce new wire, only high-conductivity (highly pure) scrap...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980323
EISBN: 978-1-62708-342-3
.... They are designed accordingly and built to meet the needs of the operator. 6.1.1 Machinery for Direct Extrusion The design of a direct-extrusion press is determined by the following factors: Product Aluminum and aluminum alloys (light metal) easy to extrude and/or difficult to extrude. Wire, bar...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170520
EISBN: 978-1-62708-297-6
... and Zinc Alloys Zinc, in pure form or with small alloying additions, is used in three main types of wrought products: flat-rolled products, wire-drawn products, and extruded and forged products. Wrought zinc is readily machined, joined, and finished. Properties of selected wrought alloys are listed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270053
EISBN: 978-1-62708-301-0
... of their art treasures. Holograms are also used for similar identification. Telegraphic Wires Another common crime is theft of telegraphic wires for their expensive copper content. Such cases are resolved in courts by a combination of tests. When a piece of stolen telegraphic wire is recovered from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... are obtained. This transverse weld in soft solders has to be capable of withstanding the drawing loads during the reduction in diameter of the extruded wires on multispindle drawing machines. Semifinished products in tin materials including bar, wire, tubes, and sections are produced on direct extrusion...