1-20 of 47 Search Results for

Waspaloy

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040247
EISBN: 978-1-62708-300-3
..., 706 and Various Derivatives, Loria E.A. , Ed., TMA . [Shen et al., 1995] Shen G. , et al. , “ Modeling Microstructural Development during the Forging of Waspaloy ,” Met. Trans. A. , p 1795 - 1802 . [Shen and Hardwicke, 2000] Shen G. , and Hardwicke C. , “ Modeling...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000117
EISBN: 978-1-62708-313-3
... 2.5 5 18 3 1.5 … … … … … 0.13 0.08 … … … … … … UDM56 (a) … 5 64 4.5 2 16 1.5 6 … … … … 0.07 0.02 0.03 … … … … … 0.5 UM-F13 (a) … 6.8 59 5.6 … … … 4.3 … 6.3 3.7 14 … … … … … … … … … Waspaloy (a) 1 13.5 58 1.2 3 19.5 4.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040257
EISBN: 978-1-62708-300-3
... Associated with High Temperature Deformation of Waspaloy and Inconel 718, ” Metallurgical Transactions A , Vol. 12 , 1981 , p 1655 – 1666 . 10.1007/BF02643571 [Hoffelner et al., 1982] Hoffelner W. , Wuthrich C. , Schroder G. , Gessinger G.H. , “ TZM Molybdenum as a Die...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280091
EISBN: 978-1-62708-267-9
..., and the cobalt alloy Haynes Alloy 25 (also known as L-605) made their way into the pipeline. Eventually, superalloys such as HA-188 (cobalt-base) and C-263 (nickel-base) made their way into the sheet alloy field. Wrought alloys such as A-286, IN-901, various Nimonic compositions, Waspaloy, and Astroloy were...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280211
EISBN: 978-1-62708-267-9
...) Waspaloy 4.25 0.420 1400 (760) Rene 41 4.85 0.520 1400 (760) U-500 6.00 1.00 1500 (816) U-700 7.50 1.30 1800 (982) MAR-M-200 7.00 2.50 2000 (1093) Notch-rupture testing of IN-718 nickel-base superalloy after varying solution treatments and intermediate heat treatments. All...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280323
EISBN: 978-1-62708-267-9
...) Nimonic 263 … 1670–1695 (910–925) Rene 41 2250 (1230) 1925–1960 (1050–1070) U-500 2300 (1260) 1920–2010 (1050–1100) Waspaloy 2425 (1330) 1875–1900 (1025–1040) M-252 … 1850 (1010) IN-100 … 2155–2190 (1180–1200) (a) Intended to indicate general trends in alloys. See Table...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240563
EISBN: 978-1-62708-251-8
...   Nimonic 95 19.5 53.5 18.0 … … … 2.9 2.0 <5.0 <0.15 +B+Zr   René 95 14.0 61.0 8.0 3.5 3.5 3.5 2.5 3.5 <0.3 0.16 0.01 B, 0.5 Zr   Waspaloy 19.5 57.0 13.5 4.3 … … 3.0 1.4 <2.0 0.07 0.006 B, 0.09 Zr Iron-nickel base Solid-solution hardened   19-9...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280135
EISBN: 978-1-62708-267-9
...) … 1135 2075 4 Waspaloy (c) (c) … 1010 1850 4 Cobalt-chromium-nickel-base alloys L-605 (HS-25) (f) (f) … 1230 2250 1 N-155 (HS-95) (f) (f) … 1230 2150 … S-816 (f) (f) … 1205 2200 1 (a) Minimum hardness is achieved by cooling rapidly from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280025
EISBN: 978-1-62708-267-9
... is spherical in iron-nickel-base and in some of the older nickel-base alloys, such as Nimonic 80A and Waspaloy. In the more recently developed nickel-base alloys, γ′ is generally cuboidal. Experiments have shown that variations in molybdenum content and in the aluminum/titanium ratio can change the morphology...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000009
EISBN: 978-1-62708-313-3
..., making them ideal for the most demanding applications, such as turbine blades. Wrought nickel-base superalloys are often used where high toughness is required, such as turbine discs and forged blades. Examples of the wrought alloys include Udimet 700, Rene 41, Waspaloy, N-901, and Udimet 630. Castings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280339
EISBN: 978-1-62708-267-9
... strength and improved the efficiency of hardener additions, such as titanium and aluminum. Consequently, existing superalloys, for example, Waspaloy, gained significant amounts of strength by application of the vacuum melting process. Concurrently, the availability of vacuum melting made a new generation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... 0.14 … 54 12.5 1.0 0.24 22 … 9 … Inconel 718 0.08 0.35 bal 0.015 0.35 0.3 50–55 1.0 0.2–0.8 0.65–1.15 17.0–21.0 4.75–5.5 2.8–5.5 (d) Rene 41 (AMS 5800) 0.12 0.1 5.0 0.015 0.5 … bal 10.0–12.0 1.4–1.6 3.0–3.3 18.0–20.0 … 9.0–10.5 (e) Waspaloy (AMS 5828C...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000001
EISBN: 978-1-62708-313-3
.... One of the most common phenomena observed is the “bowing” of the airfoil due to creep deformation. Typical alloys selected for the vane assembly are Waspaloy, X-40, alloy 713, MAR-M 302, B-1900, and columnar-grained MAR-M 200. Turbine blades are exposed to the hot gas stream and are subject to hot...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... 0.35 1.5 Ta, 0.015 B, 0.1 Zr Waspaloy N07001 19.5 57.0 13.5 4.3 … … 3.0 1.4 2.0 max 0.07 0.006 B, 0.09 Zr Nominal compositions of cast superalloys Table 3 Nominal compositions of cast superalloys Alloy designation Nominal composition, % C Ni Cr Co Mo Fe Al B...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
... 720 Bar 1570 228 … … 1455 211 1195 173 … … 1050 152 13 … 9 Unitemp AF2-1DA6 Bar 1560 226 1480 215 1290 187 1015 147 1040 151 995 144 20 19 16 Waspaloy Bar 1275 185 1170 170 650 94 795 115 725 105 675 98 25 23 28 Iron-base A-286 Bar 1005...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060231
EISBN: 978-1-62708-343-0
... Curve for Waspaloy reduced in life by a factor of 3× Fig. 10.5 Half-cycles of thermal strain-induced hysteresis. (a) Thermal down-shock followed by equilibrium temperatures. (b) Thermal up-shock following Space Shuttle Main Engine firing Fig. 10.6 Maximum total strain range of 1.6...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
...; crystal lattice varies slightly (0–0.5%) from that of austenite matrix; shape varies from spherical to cuboidal; size varies with exposure time and temperature. γ′ is spherical in Ni-Fe-base and in some of the older Ni-base alloys, such as Nimonic 80 and Waspaloy. In more recently developed Ni-base alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000133
EISBN: 978-1-62708-313-3
...-1DA6 Bar 1560 226 1480 215 1290 187 1015 147 1040 151 995 144 20 19 16 Waspaloy Bar 1275 185 1170 170 650 94 795 115 725 105 675 98 25 23 28 Iron-base A-286 Bar 1005 146 905 131 440 64 725 105 605 88 430 62 25 19 19 Alloy 901 Bar 1205 175...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280001
EISBN: 978-1-62708-267-9
... Zr   Unitemp AF2-1DA 12.0 59.0 10.0 3.0 6.0 … 3.0 4.6 <0.5 0.35 1.5 Ta. 0.015 B, 0.1 Zr   Waspaloy 19.5 57.0 13.5 4.3 … … 3.0 1.4 2.0 max 0.07 0.006 B, 0.09 Zr Nominal compositions of cast superalloys Table 1.2 Nominal compositions of cast superalloys...