EISBN: 978-1-62708-286-0
... 1.0–1.5 … 0.70–1.25 0.045 0.030 … … 23-8N S63018 0.28–0.38 0.28–0.38 22.0–24.0 7.9–9.0 1.5–3.5 … 0.69–0.90 0.045 0.030 … … 19-9DL S63198 0.28–0.36 … 18.0–21.0 8.0–11.0 0.75–1.50 1.0–1.75 0.03–0.80 … … 0.1–0.35 Ti 0.25–0.60 Nb 20Cb-3 N08020 0.07 … 19.0–21.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... wrought stainless steels Type UNS designation Composition (a) , % C Mn Si Cr Ni P S Other Austenitic types 201 S20100 0.15 5.5–7.5 1.00 16.0–18.0 3.5–5.5 0.06 0.03 0.25 N 202 S20200 0.15 7.5–10.0 1.00 17.0–19.0 4.0–6.0 0.06 0.03 0.25 N 205 S20500 0.12...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... 21.0 20.0 20.0 3.00 2.5 1.0 … … 32.2 0.15 0.15 N, 0.2 La, 0.02 Zr Haynes 556 R30556 22.0 21.0 20.0 3.0 2.5 0.1 … 0.3 29.0 0.10 0.50 Ta, 0.02 La, 0.002 Zr 19-9 DL S63198 19.0 9.0 … 1.25 1.25 0.4 0.3 … 66.8 0.30 1.10 Mn, 0.60 Si Incoloy 800 N08800 21.0 32.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820043
EISBN: 978-1-62708-339-3
... 0.20–0.40N S36017 21–12N 0.15–0.25 1.00–1.50 0.70–1.25 20.0–22.0 10.50–12.50 0.03 0.03 0.15–0.25N S36018 23–8N 0.28–0.38 1.50–3.50 0.60–0.90 22.0–24.0 7.0–9.0 0.04 0.015 0.28–0.35N; 0.50Co S63198 19–9DL 0.28–0.35 0.75–1.50 0.03–0.8 18.0–21.0 8.0–11.0 0.040 0.030 1.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976