1-18 of 18 Search Results for

UNS S31703

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310243
EISBN: 978-1-62708-286-0
.... This factor alone is reason to choose duplex over austenitic alloys such as 316L (UNS S31603) or 317L (UNS S31703). An equally decisive factor is strength. With codes permitting the tank’s design to be based on yield strength, the use of duplex alloys—with strengths about double those of austenitic steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820099
EISBN: 978-1-62708-339-3
... of nickel in a duplex stainless steel. The resulting nickel contents, however, are sufficient to provide significant benefit in many chemical environments. As shown in Table 4 , alloy 2205 and Ferralium 255 (UNS S32550) compare favorably with type 317L (UNS S31703) and alloy 20 (UNS N08020) in a variety...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440175
EISBN: 978-1-62708-262-4
...–4.0 Mo S31703 317L 0.03 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S32100 321 0.08 2.0 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti S34700 347 0.08 2.0 1.00 17.0–19.0 9.0–13.0 0.045 0.03 10 × %C min Nb S34800 348 0.08 2.0 1.00 17.0–19.0 9.0–13.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310247
EISBN: 978-1-62708-286-0
... Nitronic 33 PREN(a) 28 28 38 39 54 38 49 36 46 47 49 39 UNS S30100 S30153 S30200 S30215 S30300 S30400 S30403 S30409 S30415 S30453 S30500 S30800 S30815 S30900 S31000 S31008 S31254 S31266 S31600 S31603 S31609 S31635 S31700 S31703 S31725 S31726 S31753 S32100 S32109 S32200 S32654 S33000 S33400 S34565 S34700...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
... 2.0 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N S31700 317 0.08 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S31703 317L 0.03 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S32100 321 0.08 2.0 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... 0.02 0.03 16.4 10.5 2.1 1.8 0.5 … … 316TI S31635 0.02 0.03 16.4 10.5 2.1 1.8 0.5 0.40 … 317L S31703 0.02 0.06 18.4 12.5 3.1 1.7 0.5 … … 317LM S31725 0.02 0.06 18.4 13.7 4.1 1.7 0.5 … … 904L N80904 0.02 0.06 19.5 24.0 4.1 1.7 0.5 1.3 Cu...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310269
EISBN: 978-1-62708-286-0
... … … 316Ti S31635 0.08 0.10 16.0–18.0 10.0–14.0 2.0 2.0–3.0 1.00 0.045 0.030 5xC to 0.70 Ti … 317 S31700 0.08 0.10 18.0–20.0 11.0–15.0 3.0–4.0 2.0 1.00 0.045 0.030 … … 317L S31703 0.03 0.10 18.0–20.0 11.0–15.0 3.0–4.0 2.0 1.00 0.045 0.030 … … 317LN S31753 0.03...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310069
EISBN: 978-1-62708-286-0
... steels Table 4 Typical compositions of corrosion-resistant austenitic stainless steels Alloy Designation C N Cr Ni Mo Mn Si Other Other 316L S31603 0.02 0.03 16.4 10.5 2.1 1.8 0.5 … … 316Ti S31635 0.02 0.03 16.4 10.5 2.1 1.8 0.5 0.40 … 317L S31703 0.02...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... Mo; 0.10–0.16 N 316N S31651 0.08 2.00 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 317 S31700 0.08 2.00 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo 317L S31703 0.03 2.00 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo 321 S32100 0.08 2.00...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310091
EISBN: 978-1-62708-286-0
... . S32750 shows virtual immunity, while in mixtures contaminated with halides its performance ranks very closely to expensive nickel-based superalloys such as N06625 and N06455. Even the lower alloyed S32205 can offer an order of magnitude improvement over S31703 in hot contaminated acetic acid. Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030045
EISBN: 978-1-62708-282-2
... Numbering System (UNS) S20910 (Nitronic 50) alloy surface immersed in natural seawater for 28 days. Source: Ref 16 Fig. 8 Filamentous and coccoidal microorganisms observed on a UNS S20910 (Nitronic 50) alloy surface immersed in natural seawater for 42 days. Source: Ref 16 Mature...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... 0.030 1.00 16.00/18.00 10.00/14.00 2.00/3.00 316N (S31651) 0.08 2.00 0.045 0.030 1.00 16.00/18.00 10.00/14.00 2.00/3.00 N 0.10/0.16 317 (S31700) 0.08 2.00 0.045 0.030 1.00 18.00/20.00 11.00/15.00 3.00/4.00 317L (S31703) 0.030 2.00 0.045 0.030 1.00 18.00/20.00...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820043
EISBN: 978-1-62708-339-3
... 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S31703 317L 0.03 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S32100 321 0.08 2.0 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti S34700 347 0.08 2.0 1.00 17.0.-19.0 9.0–13.0 0.045 0.03 10 × %C min Nb...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
...-B) 120 0.1 (4) S31603 Type 316L 1 h at 675 °C (1250 °F) Oxalic acid (A 262-A) ... (a) Ferric sulfate (A 262-B) 120 0.1 (4) S31700 Type 317 None Oxalic acid (A 262-A) ... (a) Ferric sulfate (A 262-B) 120 0.1 (4) S31703 Type 317L 1 h at 675 °C (1250 °F) Oxalic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... 0.03 1.00 18.00–20.00 11.00–15.00 3.00–4.00 … S31703 317L 0.03 2.00 0.045 0.03 1.00 18.00–20.00 11.00–15.00 3.00–4.00 … S32100 321 0.08 2.00 0.045 0.03 1.00 17.00–19.00 9.00–12.00 … Ti:5×C min 329 0.10 2.00 0.04 0.03 1.00 25.00–30.00 3.00–6.00 1.00–2.00...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1