Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... … … … 0.8Ni; bal Ti Ti-grade 13 R53413 … … … … 0.05 0.5Ni; bal Ti Ti-grade 16 R52402 … … … 0.06 … bal Ti Ti-grade 18 R56322 3 … 2.5 … 0.06 bal Ti Ti-grade 23 R56407 6 … 4 … … 0.13 max O; bal Ti Ti-grade 24 R56405 6 … 4 0.06 … 0.2 max O; bal Ti Ti-grade 26...