Skip Nav Destination
Close Modal
Search Results for
UNS N06600
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-17 of 17
Search Results for UNS N06600
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Effects of Metallurgical Variables on the Corrosion of High-Nickel Alloys
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
.... This was corroborated through potentiodynamic anodic polarization ( Ref 23 ) and through corrosion immersion tests in boiling HCl solutions contaminated with different levels of ferric ions ( Ref 21 ). Secondary Carbide Effect in the Resistance of UNS N06600 to SCC in High-Temperature Water Inconel 600 (UNS...
Abstract
This chapter is dedicated mostly to the metallurgical effects on the corrosion behavior of corrosion-resistant alloys. It begins with a section describing the importance of alloying elements on the corrosion behavior of nickel alloys. The chapter considers the metallurgical effects of alloy composition for heat-resistant alloys, nickel corrosion-resistant alloys, and nickel-base alloys. This chapter also discusses the corrosion implications of changing the alloy microstructure via solid-state transformation, second-phase precipitation, or cold work. It concludes with a comparison of corrosion behavior between cast and wrought product forms.
Book Chapter
Materials Selection for Corrosion Control
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... carbon contents (generally >0.04%) without carbide-stabilizing elements (titanium and niobium). Examples are AISI types 302, 304, 309, 310, 316, 317, 430, and 446. Susceptible higher-nickel alloys include alloy 600 (UNS N06600), alloy 601 (UNS N06601), alloy 800 (UNS N08800) (despite the presence...
Abstract
This chapter outlines the step-by-step processes by which materials are selected in order to prevent or control corrosion and includes information on materials that are resistant to the various forms of corrosion. The various forms of corrosion covered are general (uniform) corrosion, localized corrosion, galvanic corrosion, intergranular corrosion, stress-corrosion cracking, hydrogen damage, and erosion-corrosion. In addition, the economic importance of cost-effective materials selection is also considered.
Book Chapter
Automotive and Transportation Applications
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310225
EISBN: 978-1-62708-286-0
..., formability T439HP (UNS S43035, dual-stabilized 439) 18CrCb (DIN 1.4509, 18CrCb) 441 (DIN 1.4509) 304/304L/304H (UNS S30400, S30403, S30409) 321 (UNS S32100) 309S (UNS S30908) 310S (UNS S31008) 332Mo (S35125) 600 (N06600) 601 (N06601) 625 (N06625) Front pipe 600–800...
Abstract
This chapter is a detailed account of the applications of stainless steel in automotive and transport systems. The discussion covers exhaust systems, structural components, automotive components, trucks, and rail transport.
Book Chapter
Nickel and Nickel Alloys
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170495
EISBN: 978-1-62708-297-6
... Nicrofer 6629 (B-4) N10629 bal 0.5–1.5 1.0–6.0 2.5 26.0–30.0 … … … 0.1–0.5 0.01 1.5 0.05 … … Nickel-chromium-iron alloys Inconel 600 N06600 72.0 min (b) 14.0–17.0 6.0–10.0 … … … … … … 0.15 1.0 0.5 … 0.5 Cu Inconel 601 N06601 58.0–63.0 21.0–25.0 bal...
Abstract
This article examines the role of alloying in the production and use of nickel and its alloys. It explains how nickel-base alloys are categorized and lists the most common grades along with their compositional ranges and corresponding UNS numbers. It describes the role of nearly 20 alloying elements and how they influence strength, ductility, hardness, and corrosion resistance. It also addresses processing issues, explaining how alloying and intermetallic phases affect forming, welding, and machining operations.
Book Chapter
Corrosion Resistance of Stainless Steels and Nickel Alloys
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... ). Fig. 2 Compositional and property linkages for nickel-base alloys Nickel-Chromium Alloys By far, the largest family of nickel alloys is that based on the nickel-chromium system, with alloy 600 (N06600) being the prototype ( Fig. 2 ). Chromium imparts resistance to oxidizing environments...
Abstract
Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance of these alloys. Some categories of corrosion covered are pitting, crevice, intergranular, stress-corrosion cracking, general, and high-temperature corrosion.
Book Chapter
Corrosion of High-Nickel Alloy Weldments
Available to PurchaseBook: Corrosion of Weldments
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820125
EISBN: 978-1-62708-339-3
... (a) 0.01 (a) ... ... ... B-3 N10675 Wrought 65 (b) 0.2 (a) 28.5 1.5 1.5 3 (a) 3 (a) 0.1 (a) 0.01 (a) 0.5 (a) ... ... N-7M N30007 Cast bal ... 31.5 1 (a) 3 (a) ... 1 (a) 1 (a) 0.07 (a) ... ... ... Ni-Cr 600 N06600 Wrought 76 0.2 ... 15.5 8...
Abstract
Nickel-base alloys used for low-temperature aqueous corrosion are commonly referred to as corrosion-resistant alloys (CRAs), and nickel alloys used for high-temperature applications are known as heat-resistant alloys, high-temperature alloys, or superalloys. The emphasis in this chapter is on the CRAs and in particular nickel-chromium-molybdenum alloys. The chapter provides a basic understanding of general welding considerations and describes the welding metallurgy of molybdenum-containing CRAs and of nickel-copper, nickel-chromium, and nickel-chromium-iron CRAs. It discusses the corrosion behavior of nickel-molybdenum alloys and nickel-chromium-molybdenum alloys. Information on the phase stability and corrosion behavior of nickel-base alloys is also included.
Book Chapter
Properties of Nickel-Alloy Welds
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930329
EISBN: 978-1-62708-359-1
...-resistant nickel and nickel-base alloys All alloys air cooled or water quenched. Alloy UNS No. Temperature (a) °C °F 200 N02200 830–871 1525–1600 201 N02201 830–871 1525–1600 400 N04400 871 1600 600 N06600 925–1040 1700–1900 601 N06601 1175 2150 690 … 1040...
Abstract
Nickel-base alloys are generally used in harsh environments that demand either corrosion resistance or high-temperature strength. This article first describes the general welding characteristics of nickel-base alloys. It then describes the weldability of solid-solution nickel-base alloys in terms of grain boundary precipitation, grain growth, and hot cracking in the heat-affected zone; fusion zone segregation and porosity; and postweld heat treatments. Next, the article analyzes the welding characteristics of dissimilar and clad materials. This is followed by sections summarizing the various types and general weldability of age-hardened nickel-base alloys. The article then discusses the composition, welding metallurgy, and properties of cast nickel-base superalloys. Finally, it provides information on the welding of dissimilar metals, filler metal selection for welding clad materials and for overlay cladding, service conditions during repair, and welding procedural idiosyncrasies of cobalt-base alloys.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
... in the presence of small concentrations of oxidizing impurities. The Ni-Fe-Cr alloys, such as alloys 600 (UNS N06600) and 800 (N08800), are used widely in the power generation industry as steam generator tubing. The Ni-Fe-Cr-Mo alloys, such as alloy 825 (N08825) and alloy 2550 (N06255), are used in a variety...
Abstract
Nickel and nickel-base alloys are specified for many applications, such as oil and gas production, power generation, and chemical processing, because of their resistance to stress-corrosion cracking (SCC). Under certain conditions, however, SCC can be a concern. This chapter describes the types of environments and stress loads where nickel-base alloys are most susceptible to SCC. It begins with a review of the physical metallurgy of nickel alloys, focusing on the role of carbides and intermetallic phases. It then explains how SCC occurs in the presence of halides (such as chlorides, bromides, iodides, and fluorides), sulfur-bearing compounds (such as H2S and sulfur-oxyanions), high-temperature and supercritical water, and caustics (such as NaOH), while accounting for temperature, composition, microstructure, properties, environmental contaminants, and other factors. The chapter also discusses the effects of hydrogen embrittlement and provides information on test methods.
Book Chapter
Chemical Compositions of Alloys and Filler Metals
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... … … … Bal … … … … Cu: 55.0 CUPRO 107 … … … Bal … 0.8 … … Cu: 68.0, Mn: 1.1 INCONEL 600 N06600 0.08 (a) 15.5 Bal … 8.0 … … … INCONEL 601 N06601 0.10 (a) 23.0 Bal … 14.4 … … Al: 1.4 Nicrofer 6025HT (602CA) N06025 0.2 25 Bal … 10 … … Al: 2.1, Ti: 0.15, Y...
Abstract
This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion-strengthened alloys; and iron-, nickel- and cobalt-base filler metals.
Book Chapter
Superalloys
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... … … … … 0.75 0.58 44.8 0.35 … Nickel-base Haynes 214 N07214 16.0 76.5 … … … … … 4.5 3.0 0.03 Haynes 230 N06230 22.0 55.0 5.0 max 2.0 14.0 … … 0.35 3.0 max 0.10 0.015 max B, 0.02 La Inconel 600 N06600 15.5 76.0 … … … … … … 8.0 0.08 0.25 Cu Inconel 601...
Abstract
This article discusses the composition, structure, and properties of iron-nickel-, nickel-, and cobalt-base superalloys and the effect of major alloying and trace elements. It describes the primary and secondary roles of each alloying element, the amounts typically used, and the corresponding effect on properties and microstructure. It also covers mechanical alloying and weldability and includes nominal composition data on many wrought and cast superalloys.
Book Chapter
Oxidation
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080005
EISBN: 978-1-62708-304-1
Abstract
Many metallic components, such as retorts in heat treat furnaces, furnace heater tubes and coils in chemical and petrochemical plants, waterwalls and reheater tubes in boilers, and combustors and transition ducts in gas turbines, are subject to oxidation. This chapter explains how oxidation affects a wide range of engineering alloys from carbon and Cr-Mo steels to superalloys. It discusses the kinetics and thermodynamics involved in the formation of oxides and the effect of surface and bulk chemistry. It provides oxidation data for numerous alloys and intermetallics in terms of weight gain, metal loss, depth of attack, and oxidation rate. It also discusses the effect of metallurgical and environmental factors such as oxygen concentration, high-velocity combustion gas streams, chromium depletion and breakaway, component thickness, and water vapor.
Book Chapter
Furnaces and Related Equipment for Heat Treating
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440055
EISBN: 978-1-62708-262-4
... 0.05 16 Bal … … … 4.5 Al, 0.002–0.40 Y 230 N06230 … 0.1 22 Bal … 2 14 0.005 B, 0.02 La Incoloy 800 N08800 Bal 0.1 19–23 30–35 … … … 0.15–0.60 Al, 0.15–0.60 Ti Incoloy 802 N08802 Bal 0.2–0.5 19–23 30–35 … … … … Incoloy 600 N06600 6–10 0.15 max 14–17 72...
Abstract
This chapter, a detailed account of furnaces and related equipment for heat treating, begins by describing three basic modes of heat transmission, namely conduction, convection, and radiation, followed by a discussion on the working principle, applications, advantages, and disadvantages of furnaces classified based on the heat transfer medium employed. The types of furnaces covered are batch-type, continuous-type, liquid bath, fluidized bed, and vacuum. The subsequent sections provide information on furnace parts, fixtures, quenching mediums, and quenching systems. The final section of the chapter describes the types of atmospheres available, emphasizing their applications and limitations.
Book
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Book Chapter
Corrosion Characteristics of Structural Materials
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... A 588) used in building and bridge construction Table 2 Compositional limits for weathering steel grades (ASTM A 588) used in building and bridge construction Grade UNS designation Heat compositional limits (a) , % C Mn P S Si Cr Ni Cu V Other A K11430 0.10–0.19 0.90–1.25...
Abstract
All materials are susceptible to corrosion or some form of environmental degradation. Although no single material is suitable for all applications, usually there are a variety of materials that will perform satisfactorily in a given environment. The intent of this chapter is to review the corrosion behavior of the major classes of metals and alloys as well as some nonmetallic materials, describe typical corrosion applications, and present some unique weaknesses of various types of materials. It also aims to point out some unique material characteristics that may be important in material selection, and discuss, where appropriate, the characteristic forms of corrosion that attack specific materials. The materials addressed in this chapter include carbon steels, weathering steels, and alloy steels; nickel, copper, aluminum, titanium, lead, magnesium, tin, zirconium, tantalum, niobium, and cobalt and their alloys; polymers; and other nonmetallic materials, including rubber, carbon and graphite, and woods.
Book Chapter
The Production of Extruded Semifinished Products from Metallic Materials
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
Abstract
Compared with other deformation processes used to produce semifinished products, the hot-working extrusion process has the advantage of applying pure compressive forces in all three force directions, enhancing workability. The available variations in the extrusion process enable a wide spectrum of materials to be extruded. This chapter focuses on the processes involved in the extrusion of semifinished products in various metals and their alloys, namely tin, lead, lead-base soft solders, tin-base soft solders, zinc, magnesium, aluminum, copper, titanium, zirconium, iron, nickel, and powder metals. It discusses their properties and applications as well as suitable equipment for extrusion. It further discusses the processes involved in the extrusion of semifinished products in exotic alloys and extrusion of semifinished products from metallic composite materials.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1