... and/or a lack of appreciation of the true service conditions ( Ref 5 ). As an example, a type 316 stainless steel (Unified Numbering System, or UNS, S31600) pipe was considered a suitable choice for admitting steam and subsequently air into a chemical slurry in a reaction vessel; however, it experienced...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090043
EISBN: 978-1-62708-266-2
... A106B 0.3 C, 0.3–1.1 Mn, 0.1 Si (min) 241 35 415 60 … G41300 4130 (AISI) 0.3 C, 1 Mn, 0.25 Si, 1 Cr, 0.2 Mo 615–1358 89–197 676–1613 98–234 12–28 G43400 4340 (AISI) 0.4 C, 0.7 Mn, 0.25 Si, 0.8 Cr, 1.8 Ni, 0.25 Mo 896–1572 130–228 979–1958 142–284 11–21 K21590 A387 (22...