... and/or a lack of appreciation of the true service conditions ( Ref 5 ). As an example, a type 316 stainless steel (Unified Numbering System, or UNS, S31600) pipe was considered a suitable choice for admitting steam and subsequently air into a chemical slurry in a reaction vessel; however, it experienced...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310269
EISBN: 978-1-62708-286-0
... J92710 0.08 … 18.0–21.0 9.0–12.0 1.50 … 2.00 0.04 0.04 Nb 8XC min CF-8M 316 J92900 0.08 … 18.0–21.0 9.0–12.0 1.50 2.0–3.0 2.00 0.04 0.04 … CF-10 304H J92590 0.04–0.10 … 18.0–21.0 8.0–11.0 1.50 … 2.00 0.04 0.04 … CF-10M 316H J92901 0.04–0.10 … 18.0–21.0 9.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
... CF-3MN 316LN J92700 0.03 1.50 1.50 17.0–21.0 9.0–13.0 2.0–3.0 0.10–0.20 N CF-8 304 J92600 0.08 1.50 2.00 18.0–21.0 8.0–11.0 CF-8C 347 J92710 0.08 1.50 2.00 18.0–21.0 9.0–12.0 Nb CF-8M 316 J92900 0.08 1.50 2.00 18.0–21.0 9.0–12.0 2.0–3.0 CF-10 304H...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... 316L W 0.03 1.50 1.50 0.04 0.04 17-21 9-13 Mo 2.0-3.0 CF-8M J92900 D319(316) W 0.08 1.50 2.00 0.04 0.04 18-21 9-12 Mo 2.0-3.0 CF-8C J92710 347 W 0.08 1.50 2.00 0.04 0.04 18-21 9-12 Cb 8 × C min, 1.0 max CF-16F J92701 303 W 0.16 1.50 2.00 0.17 0.04 18-21...