Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440097
EISBN: 978-1-62708-262-4
... 15B35H H15351 0.31–0.39 0.70–1.20 0.040 0.050 0.15–0.30 15B37H H15371 0.30–0.39 1.00–1.50 0.040 0.050 0.15–0.30 15B41H H15411 0.35–0.45 1.25–1.75 (a) 0.040 0.050 0.15–0.30 15B48H H15481 0.43–0.53 1.00–1.50 0.040 0.050 0.15–0.30 15B62H H15621 0.54–0.67 1.00–1.50...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
... 0.30–0.39 1.00–1.50 0.040 0.050 0.15–0.30 15B41H H15411 0.35–0.45 1.25–1.75 (a) 0.040 0.050 0.15–0.30 15B48H H15481 0.43–0.53 1.00–1.50 0.040 0.050 0.15–0.30 15B62H H15621 0.54–0.67 1.00–1.50 0.040 0.050 0.40–0.60 (a) Standard AISI-SAE H-steels with 1.75 manganese...