... carbon steel with a manganese content of no greater than 1.0% with a mean (nominal) carbon content of 0.40 wt% carbon. Additionally, there may be equivalent designations using the Unified Numbering System (UNS) established by ASTM International (ASTM E527) and SAE International (SAE J 1086). The first...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
... steels 6118 G61180 760 (1400) 850 (1560) 775 (1430) 690 (1270) … 6150 G61500 750 (1380) 790 (1450) 745 (1370) 695 (1280) 285 (545) Silicon-manganese steels 9254 (f) G92540 766 (1410) 820 (1510) … … 275 (527) 9260 G92600 745 (1370) 815 (1500) 750 (1380) 715 (1315...