Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440125
EISBN: 978-1-62708-262-4
... 0.025 0.025 0.15–0.30 1.65–2.00 0.70–0.90 0.20–0.30 4615 G46150 0.13–0.18 0.45–0.65 0.035 0.040 0.15–0.30 1.65–2.00 … 0.20–0.30 4620 G46200 0.17–0.22 0.45–0.65 0.035 0.040 0.15–0.30 1.65–2.00 … 0.20–0.30 4626 G46260 0.24–0.29 0.45–0.65 0.035 0.040 0.15–0.30 0.70...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
... carbon steel with a manganese content of no greater than 1.0% with a mean (nominal) carbon content of 0.40 wt% carbon. Additionally, there may be equivalent designations using the Unified Numbering System (UNS) established by ASTM International (ASTM E527) and SAE International (SAE J 1086). The first...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... 1.65/2.00 0.40/0.60 0.20/0.30 4340 G43400 0.38/0.43 0.60/0.80 0.035 0.040 0.15/0.30 1.65/2.00 0.70/0.90 0.20/0.30 E4340 G43406 0.38/0.43 0.65/0.85 0.025 0.025 0.15/0.30 1.65/2.00 0.70/0.90 0.20/0.30 Ni-Mo Steels 4615 G46150 0.13/0.18 0.45/0.65 0.035 0.040 0.15/0.30...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
... 715 (1320) 820 (1510) 665/1230 580 (1080) 365 (685) 94B15 G94151 … … … … … 94B17 G94171 705 (1300) 840 (1540) 770 (1420) 640 (1180) 415 (780) 94B30 G94301 720 (1330) 805 (1485) 750 (1380) 655 (1210) 370 (695) Nickel-molybdenum steels 4615 G46150 725 (1340) 810...