Fig. 9.14 Plate martensite in water-quenched eutectoid (~0.8% C) steel (UNS G10800) The light regions between the martensite plates are retained austenite. 10% sodium metabisulfite etch. Original magnification 1000×. Source: Ref 9.6 More
Image
Published: 31 December 2020
Fig. 15 Pearlite colonies of a plain carbon UNS G10800 steel showing colonies of pearlite. 4% picral etch. Original magnification: 200×. The cementite appears dark and the ferrite light. Source: Ref 13 More
Image
Published: 01 October 2011
Fig. 9.4 Distinctive lamellar pattern of pearlite that occurs when a carbon-austenite solid solution decomposes into a ferrite-cementite mixture after very slow (near equilibrium) cooling. Plain carbon steel (UNS G10800) showing colonies of pearlite. 4% picral etch. Original magnification 200× More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440097
EISBN: 978-1-62708-262-4
... G10700 0.65–0.75 0.60–0.90 0.040 0.050 1080 G10800 0.75–0.88 0.60–0.90 0.040 0.050 1084 G10840 0.80–0.93 0.60–0.90 0.040 0.050 1090 G10900 0.85–0.98 0.60–0.90 0.040 0.050 1095 G10950 0.90–1.03 0.30–0.50 0.040 0.050 Source: Ref 1 All of the grades listed...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
... G10700 0.65–0.75 0.60–0.90 0.040 0.050 1075 G10750 0.70–0.80 0.40–0.70 0.040 0.050 1080 G10800 0.75–0.88 0.60–0.90 0.040 0.050 1090 G10900 0.85–0.98 0.60–0.90 0.040 0.050 1095 G10950 0.90–1.03 0.30–0.50 0.040 0.050 Source: Ref 2 , 3 From Table 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060197
EISBN: 978-1-62708-261-7
... a carbon-austenite solid solution decomposes into a ferrite-cementite mixture after very slow (near equilibrium) cooling. Plain carbon steel (UNS G10800) showing colonies of pearlite. 4% picral etch. Original magnification 200× Yield strength of eutectoid steels—also called pearlitic steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... * 1059 G10590 0.55/0.65 0.50/0.80 0.040 0.050 1060 G10600 0.55/0.65 0.60/0.90 0.040 0.050 1070 G10700 0.65/0.75 0.60/0.90 0.040 0.050 * 1074 G10740 0.70/0.80 0.50/0.80 0.040 0.050 1078 G10780 0.72/0.85 0.30/0.60 0.040 0.050 1080 G10800 0.75/0.88 0.60/0.90...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310029
EISBN: 978-1-62708-326-3
... Pearlite colonies of a plain carbon UNS G10800 steel showing colonies of pearlite. 4% picral etch. Original magnification: 200×. The cementite appears dark and the ferrite light. Source: Ref 13 Pearlite in a eutectoid steel is nucleated at austenite grain boundaries and grows as spherical-shaped...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
...–0.90 0.040 0.050 … G10800 1080 0.74–0.88 0.60–0.90 0.040 0.050 … G10950 1095 0.90–1.04 0.30–0.50 0.040 0.050 … Manganese-carbon G15130 1513 0.10–0.16 1.10–1.40 0.040 0.050 … G15270 1527 0.22–0.29 1.20–1.50 0.040 0.050 … G15410 1541 0.36–0.44 1.35–1.65...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.9781627083263
EISBN: 978-1-62708-326-3
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... G10800 790–815 1450–1500 1084 G10840 790–815 1450–1500 1086 G10860 790–815 1450–1500 1090 G10900 790–815 1450–1500 1095 G10950 790–815 1450–1500 1526 G15260 860–900 1575–1650 1527 G15270 860–900 1575–1650 1541 G15410 800–845 1475–1550 1548 G15480 800–845...