Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440097
EISBN: 978-1-62708-262-4
...–0.42 0.60–0.90 0.040 0.050 1040 G10400 0.37–0.44 0.60–0.90 0.040 0.050 1045 G10450 0.43–0.50 0.60–0.90 0.040 0.050 1050 G10500 0.48–0.55 0.60–0.90 0.040 0.050 1055 G10550 0.50–0.60 0.60–0.90 0.040 0.050 1060 G10600 0.55–0.65 0.60–0.90 0.040 0.050 1070...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
...–0.42 0.60–0.90 0.040 0.050 1040 G10400 0.37–0.44 0.60–0.90 0.040 0.050 1045 G10450 0.43–0.50 0.60–0.90 0.040 0.050 1050 G10500 0.48–0.55 0.60–0.90 0.040 0.050 1055 G10550 0.50–0.60 0.60–0.90 0.040 0.050 1060 G10600 0.55–0.65 0.60–0.90 0.040 0.050 1070...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... * 1059 G10590 0.55/0.65 0.50/0.80 0.040 0.050 1060 G10600 0.55/0.65 0.60/0.90 0.040 0.050 1070 G10700 0.65/0.75 0.60/0.90 0.040 0.050 * 1074 G10740 0.70/0.80 0.50/0.80 0.040 0.050 1078 G10780 0.72/0.85 0.30/0.60 0.040 0.050 1080 G10800 0.75/0.88 0.60/0.90...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
... … G10200 1020 0.17–0.23 0.30–0.60 0.040 0.050 … G10300 1030 0.27–0.34 0.60–0.90 0.040 0.050 … G10400 1040 0.36–0.44 0.60–0.90 0.040 0.050 … G10500 1050 0.47–0.55 0.60–0.90 0.040 0.050 … G10600 1060 0.55–0.66 0.60–0.90 0.040 0.050 … G10700 1070 0.65–0.73 0.60...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
...–1550 1049 G10490 800–845 1475–1550 1050 G10500 800–845 1475–1550 1053 G10530 800–845 1475–1550 1055 G10550 800–845 1475–1550 1059 G10590 800–845 1475–1550 1060 G10600 800–845 1475–1550 1070 G10700 800–845 1475–1550 1078 G10780 790–815 1450–1500 1080...