...–0.42 0.60–0.90 0.040 0.050 1040 G10400 0.37–0.44 0.60–0.90 0.040 0.050 1045 G10450 0.43–0.50 0.60–0.90 0.040 0.050 1050 G10500 0.48–0.55 0.60–0.90 0.040 0.050 1055 G10550 0.50–0.60 0.60–0.90 0.040 0.050 1060 G10600 0.55–0.65 0.60–0.90 0.040 0.050 1070...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400001
EISBN: 978-1-62708-258-7
... is G10400. The letter “G” represents the AISI/SAE plain carbon and alloy steels. Other ferrous alloys have different letters, such as “F” for cast irons and cast steels (cast steels can also have the letter “J”), “D” for steels with specific mechanical properties, “S” for heat- and corrosion-resistant...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
... 1038 G10380 0.35–0.42 0.60–0.90 0.040 0.050 1040 G10400 0.37–0.44 0.60–0.90 0.040 0.050 1045 G10450 0.43–0.50 0.60–0.90 0.040 0.050 1050 G10500 0.48–0.55 0.60–0.90 0.040 0.050 1055 G10550 0.50–0.60 0.60–0.90 0.040 0.050 1060 G10600 0.55–0.65 0.60–0.90 0.040...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
... 0.050 … G10200 1020 0.17–0.23 0.30–0.60 0.040 0.050 … G10300 1030 0.27–0.34 0.60–0.90 0.040 0.050 … G10400 1040 0.36–0.44 0.60–0.90 0.040 0.050 … G10500 1050 0.47–0.55 0.60–0.90 0.040 0.050 … G10600 1060 0.55–0.66 0.60–0.90 0.040 0.050 … G10700 1070...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... 1575–1625 1029 G10290 845–870 1550–1600 1030 G10300 845–870 1550–1600 1035 G10350 830–860 1525–1575 1037 G10370 830–860 1525–1575 1038 G10380 830–860 1525–1575 1040 G10400 830–860 1525–1575 1042 G10420 800–845 1475–1550 1043 G10430 800–845 1475–1550...