... classification of coppers and copper alloys Generic name UNS No. Composition Wrought alloys Coppers (a) C10100–C15815 > 99% Cu High-copper alloys (b) C16200–C19900 > 96% Cu Brasses C20100–28000 Cu-Zn Leaded brasses C31200–C38500 Cu-Zn-Pb Tin brasses C40400–C48600...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980567
EISBN: 978-1-62708-342-3
... 0.2 max bal CuZn39Pb3 C38500 0.1 max 0.5 max … 0.5 max 2.5–3.5 … 0.4 max 36–40.5 Others total 0.2 max bal CuZn40 C46600 0.05 max 0.2 max … 0.3 max 0.3 max … 0.2 max 37.45–40.5 Others total 0.2 max bal CuZn40Al2 C67410 1.3–2.3 1.0 max 1.4–2.6 2.0 max … 0.3–1.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310351
EISBN: 978-1-62708-326-3