1-3 of 3 Search Results for

UNS A14130

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980567
EISBN: 978-1-62708-342-3
... total 0.15 max bal AlSi10Mg A94046 9.0–11.0 0.60 max 0.10 max 0.6 max 0.15–0.40 … 0.1 max 0.05 Ni max, 0.05 Pb max, 0.05 Sn max, 0.20 Ti max bal AlSi12 A14130 11.0–13.5 0.70 max 0.10 max 0.5 max 0.10 max … 0.1 max 0.1 Ni max, 0.1 Pb max, 0.05 Sn max, 0.20 Ti max bal AlSi5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... Vanasil A03930 ... ... ... ... ... ... 413.0 13 ... A04130 ... ... ... ... ... ... A413.0 A13 ... A14130 ... ... 305 ... Al–Si12Cu 44100 B443.0 43 (high purity) ... A24430 43 S5A ... ... ... ... C443.0 43 ... A34430 43 S5C 304 ... ... ... A444.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5