Published: 01 December 2004
Fig. D3.24 A356.0-T6 aluminum casting, compressive tangent modulus curves, various casting processes Effect of molding process. Heat treatment, 12 h at 538 °C (1000 °F), water quench, 12–24 h delay at room temperature, 3 h at 154 °C (310 °F), and air cooled. UNS A13560 Source: “Mechanical More
Image
Published: 01 December 2004
: permanent mold castings, 219 MPa (31.7 ksi); sand castings, 245 MPa (35.6 ksi); insulated mold castings, 192 MPa (27.9 ksi). UNS A13560 Source: “Mechanical Properties of Premium Aluminum Casting Alloys with Various Cooling Rates,” Olin Corp., Jan 1973. As published in Cast Aluminum Section, Structural More
Image
Published: 01 December 2004
castings: ultimate tensile strength, 219 MPa (31.7 ksi); tensile yield strength, 205 MPa (29.8 ksi). UNS A13560 Source: “Mechanical Properties of Premium Aluminum Casting Alloys with Various Cooling Rates,” Olin Corp., Jan 1973. As published in Cast Aluminum Section, Structural Alloys Handbook , Vol 3 More
Image
Published: 01 December 2004
(31.5); ultimate strength MPa (ksi), X, 283 (41.1), Y, 266 (38.6), Z, 252 (36.6); strain hardening exponent ( n ), X, 0.083, Y, 0.087, Z, 0.091; strain-hardening coefficient K , MPa (ksi), X, 388 (56.4), Y, 397 (57.6), Z, 382 (55.4). UNS A13560 Source: Fatigue and Fracture Toughness ofA356-T6 Cast More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140193
EISBN: 978-1-62708-335-5
... strength MPa (ksi), X, 283 (41.1), Y, 266 (38.6), Z, 252 (36.6); strain hardening exponent ( n ), X, 0.083, Y, 0.087, Z, 0.091; strain-hardening coefficient K , MPa (ksi), X, 388 (56.4), Y, 397 (57.6), Z, 382 (55.4). UNS A13560 Source: Fatigue and Fracture Toughness ofA356-T6 Cast Aluminum Alloy , R.I...