Skip Nav Destination
Close Modal
Search Results for
Suspension lugs
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-14 of 14 Search Results for
Suspension lugs
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270005
EISBN: 978-1-62708-301-0
...: Failure of a Hip Prosthesis Example: Machining Defect: Failure of Titanium Alloy Compressor Blades Example: Heat Treatment Defect: Cracking of a Nitrided Quill Shaft Example: Hydrogen Embrittlement: Failure of a Rocket Suspension Lug Example: Residual Stress Relief: Failure of a Long I-beam...
Abstract
This chapter identifies the primary causes of service failures and discusses the types of defects from which they stem. It presents more than a dozen examples of failures attributed to such causes as design defects, material defects, and manufacturing or processing defects as well as assembly errors, abnormal operating conditions, and inadequate maintenance. It also describes the precise usage of terms such as defect, flaw, imperfection, and discontinuity.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.9781627083010
EISBN: 978-1-62708-301-0
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
... are machined on both inside and outside areas, mainly for balancing and partially for styling. Stylists are coming up with designs that have minimum machining of the face and still create a contrast for appearance. The back of the face is not usually machined except for the lug nut mounting that creates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180151
EISBN: 978-1-62708-256-3
... to fracture. Fig. 2 Fractured lug, part of a pin-joint assembly, showing sequence of fracture. Fracture A preceded fractures B and C Fig. 11 Fracture of driveshaft propagating from built-up weld. The microstructure shows transition from weld (top) to base metal (bottom). Longitudinal...
Abstract
This appendix focuses on procedures, techniques, and precautions associated with the investigation and analysis of metallurgical failures that occur in service. It describes the steps of an orderly failure analysis from collecting and examining samples to performing mechanical and nondestructive tests, preparing and examining fractographs and micrographs, determining failure mode, writing the report, and developing follow-up recommendations. It also examines the fundamental mechanisms of failure, why they occur, and how to identify them by their characteristic features.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610549
EISBN: 978-1-62708-303-4
.... Source: Ref 1 Fig. 2 Fractured lug, part of a pin-joint assembly, showing sequence of fracture. Fracture A preceded fractures B and C. Source: Ref 1 Abstract Abstract This chapters discusses the basic steps in the failure analysis process. It covers examination procedures...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870001
EISBN: 978-1-62708-314-0
... fabrication and assembly costs; adverse effects of both temperature and moisture; poor strength in the out-of-plane direction where the matrix carries the primary load (they should not be used where load paths are complex, such as with lugs and fittings); susceptibility to impact damage and delaminations...
Abstract
This chapter covers the basic aspects of composite materials. It describes the arrangement, form, and function of their constituent materials and explains how they perform better in combination than on their own. It discusses the directional nature of isotropic, anisotropic, and orthotropic materials, the orientation of plies in unidirectional (lamina) and quasi-isotropic (laminate) lay-ups, and the dominant role of fibers in determining strength, stiffness, and other lamina properties. The chapter also compares the engineering attributes of composites with those of metals and includes application examples.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320049
EISBN: 978-1-62708-332-4
... and the attached members. The assembly includes an independent suspension with a spring-loaded McPherson strut attached to the upper part of the knuckle by bolting at two locations. The lower part is attached to the lower control arm through a ball joint. The lower control arm is mounted on the chassis frame...
Abstract
This chapter provides an overview of how the disciplines of design, material, and manufacturing contribute to engineering for functional performance. It describes the interaction of product designers and casting engineers in product development. It discusses the consequences of component failure, uncertainty in data and assumptions, and selection of the factor of safety. The chapter also presents an overview of the functional requirements for product performance and provides an overview of product design development. It also presents a partial list of the different tests that are performed on prototypes and examples of product testing. The chapter describes the requirements of a traceability system.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320217
EISBN: 978-1-62708-332-4
Abstract
Steel is broadly classified as plain-carbon steels, low-alloy steels, and high-alloy steels. This chapter begins by describing microconstituents of low- and medium-carbon steel, including bainite and martensite. This is followed by a section discussing the effect of alloying elements on steel. Then, it provides an overview of steel casting applications. Next, the chapter reviews engineering guidelines for steel castings and feeder design. The following section provides information on feeding aids. Further, the chapter describes the elements of gating systems for steel castings. It also describes the alloys, properties, applications, and engineering details of steel. Finally, the chapter explains defects in steel castings and presents guidelines for problem solving with examples.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... be 4D , but this distance can be increased if the dominant load is tension, such as on a pressure vessel port. The 2D edge distance can be decreased on boss or lug design if the hole is checked for shear tear-out. In thin riveted sheets, such as aircraft panels, inter-rivet sheet buckling can occur...
Abstract
This chapter presents a comprehensive coverage of mechanical fastening methods. It begins with a discussion on the advantages and disadvantages of mechanical fastening followed by sections providing information on mechanically fastened joints and the selection of the correct fastener system. The chapter then describes important structural fasteners, namely bolts, screws, pins, collar fasteners, rivets, blind fasteners, machine pins, and spring clip fasteners. The following sections describe the process involved in presses, shrink fits, hole generation, and fastener installation. The chapter ends with information on miscellaneous mechanical fastening methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... and usually high fabrication and assembly costs. Composites are adversely affected by both temperature and moisture. Composites are weak in the out-of-plane direction where the matrix carries the primary load and should not be used where load paths are complex (e.g., lugs and fittings). Composites...
Abstract
Polymer-matrix composites are among the lightest structural materials in use today. They are also highly resistant to corrosion and fatigue and their load-carrying capabilities, such as strength and stiffness, can be tailored for specific applications. This chapter discusses the primary advantages and disadvantages of polymer-matrix composites, how they are produced, and how they perform in different applications. It describes the construction of laminates, the fibers and resins used, and the methods by which they are combined. It explains how strength, modulus, toughness, and high-temperature and corrosion behaviors are determined by the orientation, shape, and spacing of fibers, the number of plies, resin properties, and consolidation and forming methods. The chapter also covers secondary fabrication processes, such as thermoforming, machining, and joining, as well as production equipment and product forms, and include guidelines for optimizing tradeoffs when selecting fibers, resins, and production techniques.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.9781627083409
EISBN: 978-1-62708-340-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.9781627083447
EISBN: 978-1-62708-344-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9