Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
... Process Process pressure Maximum equipment pressure Maximum size Pressure limited Ribs Bosses Vertical walls Spherical shape Box sections Slides/cores Weldable Good finish, both sides Varying cross section MPa ksi MN tonf m 2 ft 2 Thermoplastics Injection 15–45 2–7 30...