Published: 01 August 2012
Fig. 16.12 (a) Hard-chrome-coated Carmo die after 50,000 stampings. (b) Physical vapor deposition CrN-coated Carmo die after 1,200,000 stampings. Source: Ref 16.7 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500133
EISBN: 978-1-62708-317-1
... Abstract Hot stamping is a forming process for ultrahigh-strength steels (UHSS) that maximizes formability while minimizing springback. This chapter covers several aspects of hot stamping, including the methods used, the effect of process variables, and the role of finite-element analysis...
Image
Published: 30 June 2023
Fig. 12.16 Stamped 5 xxx alloy automotive panel showing extensive Lüders bands after forming More
Image
Published: 30 June 2023
Fig. 12.17 Single-stamping body side of 2012 Range Rover. Dimensions of the original blank were 3465 by 1372 mm More
Image
Published: 01 January 2015
Fig. 12.31 Schematic representation of the steps involved in hot stamping. The part, formed hot in the austenitic condition, is quenched in the die to martensite. Courtesy of Ronald Hughes, SeverStal North America More
Image
Published: 01 September 2008
Fig. 25 Quench crack promoted by the presence of a deep, sharp stamp mark in a die made of AISI S7 tool steel. Source: Ref 16 More
Image
Published: 01 August 2013
Fig. 13.3 Stamping of a sheet metal part. Note that the restraint from the draw beads in the blank holder promotes more stretching of the sheet. Source: Ref 13.2 More
Image
Published: 01 August 2012
Fig. 5.23 Heating systems for industrial stamping tooling. Source: Ref 5.17 More
Image
Published: 01 August 2012
Fig. 6.26 Schematic illustrating monoblock design made from casting for stamping tooling construction. Source: Ref 6.18 More
Image
Published: 01 August 2012
Fig. 7.1 Components manufactured using hot stamping. Source: Ref 7.1 More
Image
Published: 01 August 2012
Fig. 7.2 Direct method of hot stamping. Source: Ref 7.6 More
Image
Published: 01 August 2012
Fig. 7.3 Indirect method of hot stamping. Source: Ref 7.6 More
Image
Published: 01 August 2012
Fig. 7.10 Schematic of testing machine used to determine friction in hot stamping. Source: Ref 7.10 More
Image
Published: 01 August 2012
Fig. 7.27 Hot stamping process using resistance heating. Source: Ref 7.29 More
Image
Published: 01 August 2012
Fig. 8.28 Comparison of cost per part from stamping and sheet hydroforming for different annual production volumes. More
Image
Published: 01 August 2012
Fig. 8.29 Comparison of the cost per part in stamping and sheet hydroforming for manufacturing 15 different parts More
Image
Published: 01 August 2012
Fig. 2.21 Principles of hot stamping (heating in furnace/forming and quenching in press) More
Image
Published: 01 August 2012
Fig. 7.4 Comparison of stamping processes with (a) wet lubricants and (b) dry-film lubricants. Source: Ref 7.11 More
Image
Published: 01 August 2012
Fig. 7.5 Various Tribotests used for evaluating stamping lubricants; Region 1, flange deformation; Region 2, bending and undbending; Region 3, bending and stretching; Region 4, large friction with little deformation. More
Image
Published: 01 August 2012
Fig. 12.25 Hot stamping cycle time of a direct-driven and accumulator-driven hydraulic press. Source: Ref 12.34 More