1-19 of 19 Search Results for

Sewage

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 December 2006
Fig. 2.54 Extruded blanks in AlMgSi0.5 for rotors of the air compressor of a pneumatic tanker pumping unit for sewage. Source: Honsel More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220077
EISBN: 978-1-62708-341-6
... components of differing voltages and the resultant failure of these components. In addition, any technique that reduces water consumption will provide an economic means of cutting water and sewage costs. In perhaps the simplest type of cooling system ( Fig. 5.1 ), water is passed from a tank, through...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410247
EISBN: 978-1-62708-280-8
... valves Die casting 380, 383 Diesel engine pistons Gravity permanent mold casting 332 T5 Hinges Die casting 360 F Chemical and sewage Vats, valves, and piping Air set sand casting, semi-permanent mold casting 514 F Cookware Utensils, pots and pans, waffle irons Die casting 443 F...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
... T61, T62 Chemical and sewage fittings, dairy and food handling, marine fittings, refrigerator parts, and marine parts … X … X (Elongation) … … … … XX … A 514 B 514 F F Automotive diesel pistons … … … … X … X … … X 332/333 T5,T6 T7 5.10 Product Functional Needs...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... for water and sewage. Gray cast iron gets its name from its fracture appearance. A longtime quality-control technique for cast irons was to cast a test sample, break it, and rate the fracture appearance. A uniform gray fracture meant that all went well with the casting operation. Ductile iron is used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... and industrial, the large organisms are missing, but there are still many microorganisms, such as bacteria and algae. MIC has been documented for metals exposed to process chemicals, foods, soils, aircraft fuels, human plasma, and sewage, in addition to seawater and freshwater. In all these environments...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320163
EISBN: 978-1-62708-332-4
... ductile iron as the material of choice for several structural components and heat, corrosion, and wear resistance applications. Water and sewage pipes constitute nearly 50% of the tonnage of all applications. Several critical safety components in the automotive field are made from ductile iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
... are a problem or potential problem for a product, mechanism, operation (like mining or farming), device or facility (like a sewage treatment facility), then something should be done to mitigate tribological costs. The options are: Solve existing or potential problems with existing tribological information...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030184
EISBN: 978-1-62708-282-2
... and industrial area. There are commercial, industrial, chemical, and sewage pollutants. The water samples taken at three different locations show an average resistivity of 30 Ω · cm. Fig. 22 Example 2. Outline of H-pile pier protected using a protective coating and impressed-current anodes...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030045
EISBN: 978-1-62708-282-2
... environments soured by sulfate-reducing-bacteria (SRB)-produced sulfides Underground pipeline Water-saturated clay-type soils of near-neutral pH with decaying organic matter and a source of SRB Water treatment Heat exchangers and piping Sewage handling and treatment Concrete and reinforced-concrete...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170351
EISBN: 978-1-62708-297-6
...; marine fittings; tire molds; carburetor bodies 514.0 Fittings for chemical and sewage use; dairy and food handling equipment; tire molds A514.0 Permanent mold casting of architectural fittings and ornamental hardware 518.0 Architectural and ornamental castings; conveyor parts; aircraft...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390100
EISBN: 978-1-62708-459-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
...; street lamp housings 443.0 Cookware; pipe fittings; marine fittings; tire molds; carburetor bodies 514.0 Fittings for chemical and sewage use; dairy and food handling equipment; tire molds A514.0 Permanent mold casting of architectural fittings and ornamental hardware 518.0 Architectural...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6