1-20 of 873 Search Results for

Pressurizing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1996
DOI: 10.31399/asm.tb.phtpclas.t64560406
EISBN: 978-1-62708-353-9
...Abstract Abstract This appendix contains the metric stress or pressure readings (MPa or ksi) to be converted. This appendix is a reprint of a table giving stress or pressure value conversions. Reproduced from Metal Progress Databook , American Society for Metals, Metals Park, OH (1977...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860115
EISBN: 978-1-62708-338-6
...Abstract Abstract The necessity of developing the lightest-weight structures with sufficient strength was the driving factor for the development of filament-wound composite pressure vessels. This chapter presents a brief history of the development of rocket motor cases (RMCs), followed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
...Abstract Abstract This chapter discusses various factors pertinent to the applications of low-pressure permanent mold casting process, namely decorative automotive wheels, critical safety structural components, and chassis components. low-pressure permanent mold castings decorative...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.9781627082853
EISBN: 978-1-62708-285-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270067
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed in service, causing extensive engine damage. A section of the blade broke off around 25 mm from the root platform, producing a flat fracture surface that appeared smooth on one end and grainy elsewhere. Based on their examination...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270138
EISBN: 978-1-62708-301-0
...Abstract Abstract A high-pressure turbine blade in an aircraft engine failed prematurely, fracturing close to the root. Visual examination revealed significant plastic deformation on the leading edge of the blade, blocky cleavage on the trailing edge, and a region covered with fissures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270143
EISBN: 978-1-62708-301-0
...Abstract Abstract A low-pressure turbine rotor blade failed during a test run, causing extensive damage to an aircraft engine. Visual examination showed that the nickel-base superalloy blade broke above the root platform in the airfoil section, leaving a fracture surface with two distinct...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220475
EISBN: 978-1-62708-259-4
... extends for more than 50 mm (2 in.). The location of test specimens to evaluate the process are indicated. Etchant: hot hydrochloric acid. Abstract Abstract This chapter discusses the properties and compositions of steels used in pressure vessels, piping, boilers, rebar, and other structural...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460173
EISBN: 978-1-62708-285-3
...Abstract Abstract Increasing growth of high-pressure cold spraying applications on the industrial scale have forced global powder producers to face this challenge and develop specific powders for cold spray applications. This chapter provides information on the properties, classification...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490329
EISBN: 978-1-62708-340-9
...Abstract Abstract This chapter covers the failure modes and mechanisms of concern in hydroprocessing reactor vessels and the methods used to assess lifetime and performance. It begins with a review of the materials used in the construction of pressure-vessel shells, the challenges they face...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200233
EISBN: 978-1-62708-354-6
...Abstract Abstract The design stresses for most pressure-containing structural application, which are based upon minimum mechanical properties designated in the specifications published by the American Society for Testing and Materials (ASTM). This chapter reviews metallurgical characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860019
EISBN: 978-1-62708-338-6
...Abstract Abstract This chapter outlines a methodology for the design of cylindrical pressure vessels, with emphasis on the establishment of winding patterns and the interaction between the real fiber bed geometry (finite roving dimensions) and the theoretical one. To highlight the materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460001
EISBN: 978-1-62708-285-3
... spray process technologies, namely high-pressure cold spray (HPCS) and low-pressure cold spray (LPCS), explaining differences of LPCS from HPCS. It summarizes the historical background of the cold spray process. The growing international interest in the cold spray process from the early 2000s is also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460017
EISBN: 978-1-62708-285-3
...Abstract Abstract This chapter reviews the current understanding of high-pressure cold spraying for different materials, covering widely accepted general mechanisms for particle deposition and the processes and parameters involved. It begins by reviewing the mechanisms of bonding. An overview...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460067
EISBN: 978-1-62708-285-3
...Abstract Abstract The modeling and simulation activities in the field of high-pressure cold spray can be divided into two main parts: solid mechanics and fluid dynamics. This chapter focuses on these parts of modeling work in cold spray research. The discussion covers the objective, principal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460107
EISBN: 978-1-62708-285-3
...Abstract Abstract This chapter provides an overview of the state of the art in high-pressure cold spray equipment, including both spray systems and gas supply systems. The chapter describes the commercial cold spray systems developed by companies such as Cold Gas Technology (CGT) GmbH, Plasma...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460121
EISBN: 978-1-62708-285-3
... that are used in high-pressure cold spray coating characterization, including residual-stress characterization. The chapter includes some preliminary screening of tool hardness and bond adhesion strength, as well as a distinction between surface and bulk characterization techniques and their importance for cold...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460185
EISBN: 978-1-62708-285-3
.... Coat. Technol. , Vol 204 , 2010 , p 2499 – 2503 10.1016/j.surfcoat.2010.01.031 7.17 Li Y. , Li C.-J. , Yang G.-J. , and Xing L.-K. , Thermal Fatigue Behavior of Thermal Barrier Coatings with the MCrAlY Bond Coats by Cold Spraying and Low-Pressure Plasma Spraying...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
...Abstract Abstract This chapter discusses the application of high-pressure cold spray to the automotive industry field, with special attention to three applications: additive manufacturing, fabrication methods, and protective coatings. Various studies on the automotive application of cold spray...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
...Abstract Abstract High-pressure cold spray repair process has been used on a number of different applications in the defense industry. This chapter describes various applications for cold spray systems that have operating pressures greater than 2.4 MPa (350 psi) and operating temperatures...