Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250077
EISBN: 978-1-62708-345-4
... Abstract Plastic gears are continuing to displace metal gears in applications ranging from automotive components to office automation equipment. This chapter discusses the characteristics, classification, advantages, and disadvantages of plastics for gear applications. It provides a comparison...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780055
EISBN: 978-1-62708-281-5
... for predicting plastic part performance (stiffness, strength/impact, creep/stress relaxation, and fatigue) integrated with manufacturing concerns (flow length and cycle time) are demonstrated for design and material selection. plastics material selection materials design plastic parts stiffness impact...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550325
EISBN: 978-1-62708-307-2
... Abstract This chapter describes the molecular structures and chemical reactions associated with the production of thermoset and thermoplastic components. It compares and contrasts the mechanical properties of engineering plastics with those of metals, and explains how fillers and reinforcements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780003
EISBN: 978-1-62708-281-5
... Abstract This introductory article describes the various aspects of chemical structure and composition that are important to an understanding of polymer properties and their eventual effect on the end-use performance of engineering plastics, namely thermoplastics and thermosets. The most...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
... of polymers are then discussed. The article further includes a case study describing the tribological performance of nylon. It ends by presenting some examples of wear failures of plastics. wear elastomers thermosets glassy thermoplastics semicrystalline thermoplastics lubricants nylon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060137
EISBN: 978-1-62708-355-3
... Abstract The testing of plastics includes a wide variety of chemical, thermal, and mechanical tests. This chapter reviews the tensile testing of plastics, which has been standardized in ASTM D 638, "Standard Test Method for Tensile Properties of Plastics," and other comparable standards...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300301
EISBN: 978-1-62708-323-2
... Abstract This chapter covers the friction and wear behaviors of plastics and elastomers. It begins by describing the molecular differences between the two types of polymers and their typical uses. It then discusses the important attributes of engineering plastics and their suitability...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.9781627082815
EISBN: 978-1-62708-281-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700115
EISBN: 978-1-62708-279-2
... Abstract Transformation-induced plasticity (TRIP) steels are characterized by their excellent strength and high ductility, which allow the production of more complicated parts for lightweight automotive applications. This chapter provides an overview of the compositions, microstructures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700135
EISBN: 978-1-62708-279-2
... of twinning-induced plasticity steels. chemical composition microstructure heat treatment deformation mechanical properties formability twinning-induced plasticity steels TWINNING-INDUCED PLASTICITY (TWIP) steels are austenitic steels with a high manganese content of 22 to 30% and other...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780359
EISBN: 978-1-62708-281-5
... Abstract This article reviews various analytical techniques most commonly used in plastic component failure analysis. The description of the techniques is intended to make the reader familiar with the general principles and benefits of the methodologies. The descriptions of the analytical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240017
EISBN: 978-1-62708-251-8
... on the causes, nature, and impact of these defects in metals. It also describes the mechanisms that cause plastic deformation in metals. crystalline imperfections plastic deformation deformation annealing precipitation diffusion sintering point defects line defects planar defects volume defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.htpa.t53310119
EISBN: 978-1-62708-346-1
... Abstract This chapter reviews the tests and procedures used for measuring hardness of plastics and elastomers. The conventional testing methods (Rockwell, Vickers, Brinell, and Knoop) used for testing of metals are based on the idea that hardness represents the resistance against permanent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
... Abstract This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts and includes a discussion on materials and process selection methodology for plastics. The discussion covers the primary plastic processing methods and how...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780185
EISBN: 978-1-62708-281-5
... Abstract This article briefly introduces some commonly used methods of mechanical testing of plastics for determining mechanical properties, also describing the test methods and providing comparative data for the mechanical property tests. In addition, creep testing and dynamic mechanical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040017
EISBN: 978-1-62708-300-3
... Abstract This chapter discusses the role of plastic deformation in forging and the effect of strain and strain rate on metal flow. It demonstrates the use of stress tensors and shows how metal flow can be represented qualitatively by the displacement of volume elements and quantitatively...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400027
EISBN: 978-1-62708-316-4
... Abstract This chapter discusses the fundamentals of plastic deformation and the role of strain and strain rate in sheet metal forming processes. It describes the conditions associated with uniform deformation, the significance of engineering and true strain, the effect of volume constancy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400033
EISBN: 978-1-62708-316-4
... and use of forming limit curves and the extensive amount of information they provide. anisotropy flow stress formability forming limit curves plastic deformation sheet forming tensile test WHEN A MATERIAL is deformed, two types of deformation occur: elastic and plastic. The elastic phase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780028
EISBN: 978-1-62708-281-5
... of engineering plastics and commodity plastics follows, and the final section briefly outlines the most common plastics manufacturing processes. thermal properties mechanical properties physical properties engineering plastics commodity plastics chemical composition manufacturing process molecular...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040051
EISBN: 978-1-62708-300-3
.... It then explains how to determine the onset of yielding, which corresponds to the start of plastic deformation and the flow of metal within the workpiece. The chapter then goes on to present two important yield criteria, one based on shear stress (Tresca criterion), the other on distortion energy (von Mises...