1-20 of 382 Search Results for

Moisture

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780314
EISBN: 978-1-62708-281-5
... Abstract This article describes the mechanisms of moisture-induced damage in polymeric materials, covering the characteristics of important structural plastics; the effects of moisture on glass transition temperature, modulus, creep, and stress relaxation of plastic materials; and moisture...
Image
Published: 30 June 2023
Fig. 10.26 Porosity in a weld caused by moisture More
Image
Published: 01 December 2003
Fig. 5 Moisture-induced refractive index gradient More
Image
Published: 01 December 2003
Fig. 30 Effects of moisture on nylon 6/6 measured by dynamic mechanical analysis. Size, 3 mm (0.12 in.) thick, 13 mm (0.5 in.) wide, 19 mm (0.75 in.) long; programmed at 5 °C/min (9 °F/min), in nitrogen. RH, relative humidity. Source: Ref 30 More
Image
Published: 01 November 2010
Fig. 8.3 The effect of prebond moisture on bond strength. Source: Ref 3 More
Image
Published: 01 November 2010
Fig. 8.13 Effects of prebond moisture on fatigue strength. Source: Ref 8 More
Image
Published: 01 November 2010
Fig. 13.26 Accelerated moisture absorption procedure More
Image
Published: 01 November 2010
Fig. 14.5 Effect of temperature and moisture on Kevlar/epoxy strength More
Image
Published: 01 November 2010
Fig. 14.7 Effect of temperature and moisture on interlaminar shear strength More
Image
Published: 01 November 2010
Fig. 15.1 Potential moisture effects More
Image
Published: 01 November 2010
Fig. 15.2 Effect of moisture on glass transition temperature More
Image
Published: 01 November 2010
Fig. 15.4 Effects of moisture on tension and compression strength of carbon/epoxy. Source: Ref 2 More
Image
Published: 01 November 2010
Fig. 15.5 Effects of moisture on matrix-dominated properties of carbon/epoxy. Source: Ref 2 More
Image
Published: 01 November 2010
Fig. 15.6 Typical moisture absorption behavior More
Image
Published: 01 November 2010
Fig. 15.7 Moisture absorption as a function of humidity. Source: Ref 4 More
Image
Published: 01 November 2010
Fig. 15.8 Moisture absorption as a function of temperature More
Image
Published: 01 November 2010
Fig. 15.9 Moisture absorption profiles as a function of thickness. Source: Ref 1 More
Image
Published: 01 November 2010
Fig. 15.10 Moisture absorption and desorption for carbon/epoxy More
Image
Published: 01 November 2010
Fig. 15.12 Moisture absorption for thermosets and thermoplastics. C/BMI, carbon/bismaleimide; C/E, carbon/epoxy More
Image
Published: 01 November 2010
Fig. 15.14 Effects of thermal spiking on moisture absorption of carbon/epoxy. Source: Ref 6 More