1-20 of 229 Search Results for

Marine engines

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2022
Fig. 7.35 Cut section of a marine diesel engine cylinder block More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340325
EISBN: 978-1-62708-427-7
... for the new H321 marine temper requires that metal pass a laboratory test to demonstrate that, in a sensitized state, it will not experience severe grain boundary attack. Alloys for Outboard Engines Another issue encountered in the marine environment is the potential for corrosion or damage to aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410001
EISBN: 978-1-62708-280-8
... Brake master cylinders Brake calipers ABS housings Corrosion resistance Advantages include: Minimum property deterioration with time Reduced maintenance costs Improved aesthetic appeal Anodizing and clear coating can enhance corrosion resistance. Marine engine propeller Aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080249
EISBN: 978-1-62708-304-1
... on the hot-section components, such as nozzle guide vanes and rotor blades, resulting in accelerated oxidation (or sulfidation) attack. This is commonly referred to as “hot corrosion.” Sulfur in the fuel is generally limited to 0.3% for commercial jet engines and to 1.0% for marine gas turbines ( Ref 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310243
EISBN: 978-1-62708-286-0
... Marine Systems Applications Summary AS RECENTLY AS THE 1960s AND 1970s, handbooks on stainless steel were stating that stainless steels are not stainless in seawater, and successful prolonged corrosion-free service of stainless steel in seawater requires sophisticated corrosion engineering...
Image
Published: 01 December 2006
Fig. 7.51 Porthole die for the production of the AlMgSi0.5 hollow section shown in front of the die for a water-cooled exhaust duct from a marine diesel engine. Left, mandrel; right, die plate. Source: Alusuisse More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
..., lawn mower parts X X X … … … … 380 A 380, 383 F Outboard marine parts, instrument panels, irrigation parts, aircraft parts X X … … … … … 360 A 360 F Auto transmission, pulleys, motor body and end shields XX XX … … … … … 384 F Cylinder blocks, IC engine pistons...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
.... Unlike resin-matrix composites, they are nonflammable, do not outgas in a vacuum, and suffer minimal attack by organic fluids such as fuels and solvents. The principle of incorporating a high-performance second phase into a conventional engineering material to produce a combination with features...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480353
EISBN: 978-1-62708-318-8
... equipment, sporting goods, oil and gas production, and marine vessels. aerospace applications medical applications power utility applications titanium THE BIRTH of the commercial titanium industry occurred when U.S. companies TIMET and Rem-Cru Titanium were established in 1950...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630035
EISBN: 978-1-62708-270-9
... Handbook Supplement J811, 1962 10. Forming and Forging, Vol 14 , ASM Handbook , ASM International , 1988 , p 803 11. Ancarrow J.E. and Harrington R.L. , Main Propulsion Shafting Eccentricity Considerations , Transactions , Society of Naval Architects and Marine Engineers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270005
EISBN: 978-1-62708-301-0
... following a path along which there was excessive sulfur segregation ( Ref 11 ). 2.3.3 Failures due to Assembly Example: Misalignment: Failure of a Piston in a Marine Engine With the best component design and choice of the best material, sometimes mistakes can happen during the assembly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120005
EISBN: 978-1-62708-269-3
..., and extrusions. It was not until about 1965 that nonaerospace usage accounted for a significant fraction of the titanium production. Continued modest growth has been taking place since then in many areas, including biomedical engineering, marine and chemical applications, automotive, and sporting goods...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030005
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses some important factors involved in the atmospheric corrosion of engineering materials. The discussion begins with a description of elements necessary for the operation of a galvanic corrosion cell and corrosion reactions, followed by the types of atmospheric...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
... Electrical wiring and contacts Screw machine parts (leaded yellow brasses are one of the easiest to machine metals) Marine application (saltwater resistance) Chemical vessels (monels, etc.) Decorative items Powder metal (P/M) bearings Copper alloys are used where you must use them...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... and the classifications, designations, and grades of available product forms. It also explains how aluminum alloys are used in aerospace, automotive, rail, and marine applications as well as in building and construction, electrical products, manufacturing equipment, packaging, and consumer durables such as appliances...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430376
EISBN: 978-1-62708-253-2
... Publishing, 2011 6.28 J. Colannino, Prevent Boiler Tube Failures Part 1: Fire Side Mechanisms, Chemical Engineering Progress, Oct 1993, p 33 36 6.29 G.E. Gale, Corrosion in Boilers and Water Circulation Systems with Special Reference to Marine Installations, p 166 172, last modified 2011...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320189
EISBN: 978-1-62708-347-8
... Gears, presented at the 10th Round Table Conference on Marine Gearing, Brunnen, Switzerland, 25 26 Sept 1975 O J.R. Eagan and C.H. Shelton, Recent Test Data on Selection of Alloy Steels for Gears and Bearings, Society of Automotive Engineers (SAE) Report 720301, 1972 O H. Fugio and T. Aida, Study...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030045
EISBN: 978-1-62708-282-2
... of, or an accelerating factor in, corrosion involve localized forms of attack. One reason for this is that organisms usually do not form in a continuous film on the metal surface. The large fouling organisms in marine environments settle as individuals, and it is often a period of months or even years before a complete...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550001
EISBN: 978-1-62708-307-2
... temperature. The excellent corrosion resistance of titanium allows applications in chemical processing equipment, marine components, and biomedical implants such as hip prostheses. Titanium is an important aerospace material, finding applications as airframe and jet engine components. When it is combined...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.9781627083478
EISBN: 978-1-62708-347-8